High-performance gas turbines and aircraft engines necessitate MCrAlY (M = Ni, Co, or Ni/Co) coatings with exceptional oxidation resistance. Pre-heat-treatment can enhance the performance of MCrAlY bond coatings in the following ways: First, it reduces the porosity of the bond coating and promotes the diffusion of elements within it. Second, pre-heat-treatment allows for the formation of a continuous, dense, and moderately thick layer of pure Al2O3 scale, which helps to delay the formation of mixed oxides. Lastly, proper pre-heat-treatment can increase the grain size of the Al2O3 scale, leading to a lower growth rate of the oxide scale. Additionally, this article proposes new directions for developing more reasonable and effective pre-heat-treatment methods, laying the foundation for the creation of thermal barrier coatings (TBCs) with greater durability and higher performance.
The effect of water vapor on the stress corrosion cracking (SCC) behavior of TP439 stainless steel at 500 °C was investigated using slow strain rate tensile tests at three strain rates of 2 × 10–5/s, 2 × 10–6/s, and 2 × 10–7/s. Air was selected as a comparative blank test environment for the water vapor environment. The results showed that the tensile strength of the specimens increased significantly in air when the strain rate was decreased from 2 × 10–5/s to 2 × 10–7/s, while it decreased in water vapor. Dynamic strain aging (DSA) and SCC are the main factors contributing to the difference in tensile strength of the specimens in air and water vapor. The SCC of TP439 stainless steel in water vapor at 500 °C occurs at a strain rate of 2 × 10–7/s or even lower. Based on the SCC susceptibility index and SEM observation of specimen fracture, TP439 stainless steel exhibits a slight transgranular SCC in water vapor with low SCC susceptibility.