4 December 2015 in Science
Brighter perovskite LEDs: Organic-inorganic hybrid perovskites such as methyl ammonium lead halides are attractive as low-cost light-emitting diode (LED) emitters. This is because, unlike many inorganic nanomaterials, they have very high color purity. Cho et al. made two modifications to address the main drawback of these materials, their low luminescent efficiency. They created nanograin materials lacking free metallic lead, which helped to confine excitons and avoid their quenching. The perovskite LEDs had a current efficiency similar to that of phosphorescent organic LEDs. Science , this issue p. 1222
17 November 2015 in Small
2 March 2016 in Optics Express
We report spectroscopic characterization of Fe:ZnSe quantum dots (for 2% of Zn/Fe molar ratio) fabricated by microemulsion hydrothermal synthesis. Mid-IR photoluminescence of the 5E↔5T2 transition of Fe2+ ions over 3.5–4.5 μm spectral range was observed in Fe:ZnSe quantum dot samples and kinetics of luminescence have been characterized at temperatures of 30–300 K under direct (2.788 μm) mid-IR excitation and indirect (0.355 μm) photoionization excitation. The radiative lifetime (τrad) was estimated from these measurements to be 48 µs while lifetime at room temperature was measured to be 440 ns. This agrees closely with the behavior of bulk material.
26 July 2019 in Nanotechnology
The light to be trapped inside light-emitting diodes (LEDs) greatly affects the luminous efficiency and device lifetime. Abrupt difference in refractive index between the sapphire substrate and GaN-based LEDs causes light trapping by total internal reflection, however, its optical loss has been taken for granted. In this study, we demonstrate that nanoporous GaN can be used as a refractive-index-matching layer to enhance the light transmittance at the sapphire–GaN interface in InGaN/GaN flip-chip light-emitting diodes (FCLEDs). The porosity and the refractive index of the nanoporous GaN layer are controlled by electrochemical etching of n -type GaN layer. The optical output power of FCLEDs with the nanoporous GaN layer grown on flat and patterned sapphire substrates is increased by 355% and 65% at an injection current of 20 mA, respectively, compared with that of an FCLED without the nanoporous GaN layer. The remarkable enhancement of optical output is mostly attributed to the nanoporous GaN layer which drastically increases the light extraction efficiency by decreasing the reflection of light at the sapphire–GaN interface.
17 June 2019 in Optical Materials Express
We report temperature dependent time-resolved photoluminescence studies of Fe3+ in ZnSe polycrystals over 10–300 K temperature ranges fabricated by the post growth thermal diffusion technique. The d-d transitions of Fe3+ assigned to the 4T2(G)→6A1(S) and 4T1(G)→6A1(S) transitions are clearly identified at 528 and 627 nm, respectively, at 10 K. The observed emission peaks in the near bandgap region are red-shifted from 439 to 463 nm as the temperature increases, resulting in a temperature coefficient of 10.21×10−4 eV/K and Debye temperature = 336 K fitted by the Varshni equation. The radiative lifetime at 528 nm by time-resolved photoluminescence is evaluated as τrad = 774 ± 4 ps, activation energy (ΔEa) = 717.2 cm−1, and relaxation time rate (1/W0) = 3.1 ps.
1 June 2021 in Journal of Rare Earths