12 October 2023 in IEEE Transactions on Dielectrics and Electrical Insulation
To lower the ac losses in electrical machines, additive manufacturing (AM) has been adopted to exploit the geometrical freedom in winding design. However, AM brings about new challenges such as surface roughness and porosity which can create difficulties for post processing of the windings such as applying insulation coatings. The article investigates the influence of surface roughness (profile) of AM-processed CuCrZr as a potential candidate for electrical windings in terms of geometry, surface roughness, porosity, and oxidation on their insulation. The feasibility and characteristics of insulations applied via three processing techniques namely powder, spray, and dip coating are compared. The entire process is quantified via techniques such as computed tomography, surface profilometry, optical microscopy, X-ray photon spectroscopy, and breakdown voltage (BV) at different stages of the coating process. The study also includes coating on a commercial rectangular copper wire as a reference. The initial assessment of coatings concludes that surface roughness and the coating process are both vital determinants for the success of insulating AM components. Basic surface smoothening is needed to get rid of burs and the spray coating technique was the best among others for its capability to produce conformal coating.
2 December 2024 in Journal of Materials Science: Materials in Engineering
In dental implants, zirconia is well-known as a crown material due to its excellent acid and base resistances and appearance close to natural teeth. In addition, its extraordinary mechanical properties render zirconia to be a potential candidate as an implant component of a whole implanted tooth, if its biocompatibility can be improved to promote adhesion to natural hard tissues. This study aims to enhance the bioactivity of zirconia with the aim of improving its integration with gum bone. Hydroxyapatite is the major component of natural bone and is thus selected as the modifier to improve the bioactivity of zirconia. A series of zirconia/hydroxyapatite composites with varied compositions were prepared under different conditions in order to find the optimal composites for the target application. Various analytical technologies and mechanical tests are employed to characterise the structure and properties of resultant composites. Results show that the component ratio and sintering temperature have a significant influence on the composite properties. An increase in hydroxyapatite component tends to enhance bioactivity but decline mechanical strength. Composites containing 10 wt% of hydroxyapatite maintain sufficient mechanical strength under the optimal sintering conditions whilst possessing excellent bioactivity, demonstrating that hydroxyapatite-modified zirconia has the potential as dental implant materials. Sintering results suggest that mechanical strength is obtained at 1400 °C for 2 h for the composite containing 10 wt% of hydroxyapatite.
9 July 2024 in Research Square
Zirconia is one of the best materials for making the crown in dental implant due to its excellent acid and base resistances and appearance close to natural teeth. In addition, its extraordinary mechanical properties render zirconia to be a potential candidate as dental implant, if its biocompatibility can be improved to promote adhesion to natural tissues. This study is to enhance the bioactivity of zirconia with the aim to improve its adhesion to the gingival when it is used as the crown of the implanted tooth. Hydroxyapatite is the major component of natural bone and has very high bioactivity and thus is selected as the modifier to improve the bioactivity of zirconia. A series of zirconia/hydroxyapatite composites with varied compositions were prepared under different conditions in order to find out the optimal composites for the target application. Various analytical technologies and mechanical tests are employed to characterise structure and properties of resultant composites. Experimental results show that the component ratio and sintering temperature have significant influence on the composite properties. Increase in hydroxyapatite component tends to enhance bioactivity but decline mechanical strength. Experiments found that the composite containing 10% of hydroxyapatite retains sufficient mechanical strength as crown material whilst possesses excellent bioactivity. Sintering results suggest that the optimal mechanical strength is obtained at 1400°C for 2 hours for the composite containing 10% of hydroxyapatite.