AlN/GaN resonant tunneling diodes grown on low dislocation density semi-insulating bulk GaN substrates via plasma-assisted molecular-beam epitaxy are reported. The devices were fabricated using a six mask level, fully isolated process. Stable room temperature negative differential resistance (NDR) was observed across the entire sample. The NDR exhibited no hysteresis, background light sensitivity, or degradation of any kind after more than 1000 continuous up-and-down voltage sweeps. The sample exhibited a ∼90% yield of operational devices which routinely displayed an average peak current density of 2.7 kA/cm2 and a peak-to-valley current ratio of ≈1.15 across different sizes.
We report on the design and fabrication of high current density GaN/AlN double barrier resonant tunneling diodes grown via plasma assisted molecular-beam epitaxy on bulk GaN substrates. A quantum-transport solver was used to model and optimize designs with high levels of doping and ultra-thin AlN barriers. The devices displayed repeatable room temperature negative differential resistance with peak-to-valley current ratios ranging from 1.20 to 1.60. A maximum peak tunneling current density (Jp) of 431 kA/cm2 was observed. Cross-gap near-UV (370–385 nm) electroluminescence (EL) was observed above +6 V when holes, generated from a polarization induced Zener tunneling effect, recombine with electrons in the emitter region. Analysis of temperature dependent measurements, thermal resistance, and the measured EL spectra revealed the presence of severe self-heating effects.
Cross-gap light emission is reported in n-type unipolar GaN/AlN double-barrier heterostructure diodes at room temperature. Three different designs were grown on semi-insulating bulk GaN substrates using molecular beam epitaxy (MBE). All samples displayed a single electroluminescent spectral peak at 360 nm with full-width at half-maximum (FWHM) values no greater than 16 nm and an external quantum efficiency (EQE) of ≈0.0074% at 18.8 mA. In contrast to traditional GaN light emitters, p-type doping and p-contacts are completely avoided, and instead, holes are created in the GaN on the emitter side of the tunneling structure by direct interband (that is, Zener) tunneling from the valence band to the conduction band on the collector side. The Zener tunneling is enhanced by the high electric fields (~5 × 106 V cm−1) created by the notably large polarization-induced sheet charge at the interfaces between the AlN and GaN.
We report the direct measurement of record fast switching speeds in GaN/AlN resonant tunneling diodes (RTDs). The devices, grown by plasma-assisted molecular-beam epitaxy, displayed three repeatable negative differential resistance (NDR) regions below a bias of +6 V. A room temperature peak-to-valley current ratio (PVCR) > 2 was observed, which represents a marked improvement over recent reports. Measurements carried out on hundreds of devices, of varying sizes, revealed a yield of ∼90%. Repeatability measurements consisting of 3000 sweeps resulted in a standard deviation, relative to the mean, of < 0.1%. Temperature dependent measurements combined with non-equilibrium Green's function based quantum transport simulations suggest the presence of both three-dimensional (3D) and two-dimensional (2D) emitters, giving rise to three NDR regions. Finally, a valley current density vs perimeter-to-area-ratio study indicates the presence of a surface leakage current mechanism, which reduces the PVCR.
We report on the first successful demonstration of selective deuteron acceleration by the target normal sheath acceleration mechanism in which the normally overwhelming proton and carbon ion contaminant signals are suppressed by orders of magnitude relative to the deuteron signal. The deuterium ions originated from a layer of heavy ice that was deposited on to the rear surface of a 500 nm thick membrane of Si3N4 and Al. Our data show that the measured spectrum of ions produced by heavy ice targets is comprised of ∼99% deuterium ions. With a laser pulse of approximately 0.5 J, 120 fs duration, and ∼5×1018Wcm-2 mean intensity, the maximum recorded deuterium ion energy and yield normal to the target rear surface were 3.5 MeV and 1.2×1012sr−1, respectively.