1 January 2020 in Green Processing and Synthesis
Graphene oxide hydrosol was added dropwise to the surface of chitosan (CS) to successfully obtain graphene oxide/chitosan composite (GC). The composite material was characterized by scanning electron microscopy and X-ray diffraction. The prepared adsorbent was used to simulate the static adsorption of copper, lead, and cadmium ions from 100 mL of 50 mg/L simulated wastewater samples. When the pH of the simulated wastewater is 6, initial dosage is 70 mg, adsorption time is 90 min, and temperature is 20°C; the adsorption capacities for copper, lead, and cadmium are 60.7, 48.7, and 32.3 mg/g, respectively. The adsorption and desorption cycle experiments show that the adsorption capacity of GC for copper ions can reach 86% of the initial adsorption capacity after ten cycles. The adsorption of lead ions on the composite conforms to the Freundlich adsorption isotherm model.
22 February 2023 in ACS Applied Materials & Interfaces
27 December 2021 in ACS Omega
Biomass is a promising carbon source for supercapacitor electrode materials due to its abundant source, diversity, and low-cost. Yeast is an elliptic unicellular fungal organism that is widespread in nature. In this work, we used yeast as the carbon source and Na2SiO3 as the activator to prepare a honeycomb porous carbon with higher surface area. The yeast and Na2SiO3 were directly mixed and ground without any solvent, which is simple and characterized by large-scale application. The prepared porous carbon shows a good specific capacity of 313 F/g in 6 M KOH at a density of 0.5 A/g and an excellent rate capability of 85.9% from 0.5 to 10 A/g. The results suggest that the yeast-derived porous carbon may be a promising sustainable bio-material for the preparation of supercapacitor carbon electrode materials. This study provides an economical and practical avenue for yeast resource utilization and develops a simple approach to prepare porous carbon materials.
23 March 2015 in International Journal of Energy Research
Formed activated carbon was prepared by extruding of a mixture of fine blue-coke and organic additives and subsequent carbonization and steam activation. The conditions for preparation of activated carbon were optimized with orthogonal experiments taking carbonization temperature, activation temperature, activation time and water vapor flow as influential factors, and iodine number, compressive strength and yield as indexes. The results show that the iodine number is 1157.4 mg/g, the compressive strength is 9.9 MPa and yield is 34.15%, when the activated carbon produced at the optimum conditions of 450 °C carbonization temperature, 900 °C activation temperature, 90 min activation time and water vapor flow of 50 mL/h. Meanwhile, the nitrogen adsorption isotherm and morphology are analyzed, finding the activated carbon with developed mesopores. The function groups, mainly hydroxyl and carbonyl group on activated carbon, are found by Fourier transform infrared spectroscopy. The microcrystalline structure and the degree of graphitization of the formed activated carbon are smaller than fine blue-coke by X-ray diffraction analysis. Copyright © 2015 John Wiley & Sons, Ltd.
5 November 2024 in Industrial & Engineering Chemistry Research
16 January 2020 in Water, Air, & Soil Pollution