Steel wire ropes are load-bearing components of hoisting, traction and cable systems whose degradation is concealed and cumulative, so their inspection is safety-critical. This review treats wire-rope non-destructive testing (NDT) as a materials problem, since what is measured is the state of the steel, and asks how physical sensing mechanisms, quantitative damage characterisation, data reliability and engineering standards can be integrated into one framework on which a discard decision can rest. First, degradation is mapped onto the observables that detect it through three inspection axes: the loss of metallic cross-sectional area (LMA) for distributed degradation, local flaws (LF) for broken wires, pits and cracks, and the mechanical state for damage that is neither, such as residual stress and fatigue damage. Second, three analytical results are derived and reported with their limits: a saturating magnetic-flux-leakage amplitude law for which amplitude-only depth inversion becomes severely ill-conditioned, an eddy-current skin depth that confines conventional excitation to the near surface, and a nearly non-dispersive fundamental longitudinal mode in an idealised single steel wire below 500 kHz·mm. Third, a protocol audit shows that published deep-learning figures are not comparable, and a unified evaluation protocol is proposed.
Deep-unrolled inverse-scattering networks combine physics-based iterations with learned corrections, yet stability of the trained composite is not implied by solver convergence. We analyse the layers of a Born/contrast-source formulation and turn that gap into a computable test. The layer Jacobian contains an explicit contrast-to-field coupling block, giving a state-dependent sufficient condition for non-contraction: above the threshold αc no correction confined to the contrast channel makes the evaluated layer contractive. Under β₀< 1 the field subsystem contracts, and a nonexpansive contrast projection with a positive damping floor gives the rollout an invariant bounded set; a finite-depth perturbation bound follows without assuming contraction of the composite. The weak-scattering constant β₀ follows from the acquisition operator and the contrast bound, whereas the threshold αc depends on the field state at which the layer is evaluated; both are computable before training for a reference configuration. On synthetic data β₀=0.8303< 1 while the measured spectral norm of the full layer exceeds one; experiments test the bound, the budget constraints, depth and noise. On the published Institut Fresnel geometry the test returns β₀>1, so no a-priori certificate is claimed there, and the measured reconstruction is a finite-depth evaluation with untransferred weights.