28 May 2024 in International Journal of Biological Macromolecules
3 December 2018 in Materials Research Express
Metal-assisted chemical etching (MACE) has been proposed as a promising alternative for the fabrication of micro/nano-structures on silicon with simple process and low cost. Electric field can be applied during the reaction to control the motion of charged particles so as to accelerate the reaction and form uniform vertical trenches with high aspect ratio. In this paper, boron doped p-type (100) silicon wafers with resistivity of 20~30 Ω•cm was used as substrates. A standard lift-off procedure was performed after photolithography and following deposition of layers of 5 nm Ti and 10 nm Au. The silicon substrate was then immersed into the etchant containing hydrofluoric acid (HF) and hydrogen peroxide (H2O2) with high HF-to-H2O2 concentration ratio (ρ) and an applied voltage of 40 volts. It was found that the direction of the applied electric field had a great influence on morphologies of the trenches. Deeper trenches with vertical sidewalls and relatively smoother surfaces at the bottom were observed when the silicon substrate was connected to the cathode of the power supply. Possible interpretation to these phenomena was proposed, and the effect of the electric field intensity and doping concentration was further studied.
3 May 2019 in Materials Research Express
4 February 2019 in Materials Research Express
Metal-assisted chemical etch (MACE) of silicon substrate in an etchant containing HF and H2O2 with different HF - H2O2 molar ratio R (R= [HF]/ ([HF] + [H2O2]), where [HF] and [H2O2] are the concentration of HF and H2O2 in mol/L respectively) using silver particles as catalyst was studied. Boron doped p-type (100) silicon wafers with resistivity of 0.01 Ωcm and 10.65 Ωcm were used as substrates and etched in the etchant with R = 0.7. It was found that the density of pores on the silicon substrate with resistivity of 0.01 Ωcm was higher than that with resistivity of 10.65 Ωcm. A p-type (100) silicon substrate, which was heavily and non-uniformly doped with boron, with nominal resistivity of 0.0013 Ωcm was processed by using MACE in etchant with different R's. By comparing the densities of etched pores at different doping regions, we came to the conclusion that the density of pores increased with the increase of doping concentration and with the decrease of R. It was especially obvious in the range where the pore size was smaller than the average size of silver particles. The possible reason was proposed. Finally, we used the two-point probe measurement technique to measure the resistance of this silicon substrate and verified the doping non-uniformity in the microscopic scale. This research can be applied on the detection of doping uniformity on one single wafer.