The formation of Au nanoparticles (NPs) in Au+ ion-implanted silicon nitride thin films and membranes was investigated as a function of post-implantation thermal treatments or room temperature electron irradiation at energies of 80, 120, 160, and 200 keV. The samples were characterized by Rutherford Backscattering Spectrometry and Transmission Electron Microscopy. High-temperature thermal annealing (1100 °C, 1 h) resulted in the formation of Au particles with a mean diameter of ≈1.3 nm. In comparison, room-temperature electron irradiation at energies from 80 to 200 keV caused the formation of larger Au particles according to two growth regimes. The first regime is characterized by a slow growth rate and occurs inside the silicon nitride membrane. The second regime presents a fast growth rate and starts when Au atoms become exposed to the back free surface of the membrane. Realistic binary electron-atom elastic collision cross-sections were used to analyze the observed nanoparticle growth and membrane sputtering phenomena. The results obtained demonstrate that binary electron-atom elastic collisions can account for the microstructure modifications if the critical displacement energies for the sputtering of N and Si atoms are around 14 ± 3 eV, and the displacement energy for surface located Au atoms is approximately 1.25 ± 0.2 eV. Irradiation experiments using focused electron probes demonstrate that the process provides fine control of nanoparticle formation, resulting in well-defined sizes and locations.
Single atom catalysts (SACs) appear as a promising class of materials featuring isolated metal atoms anchored to supports, where the advantages of heterogeneous catalysis are combined with a maximized noble metal atom usage. In SACs, each metal atom is fully exposed to the support surface; it is therefore critical to elucidate the nature of metal-support interface to identify the active species and design tailored, more efficient materials. Among SACs, Pt 1 /γ-Al 2 O 3 , active towards CO oxidation and isomerization of olefins, represents a prototypical system. However, the chemical complexity and poor crystallinity of γ-Al 2 O 3 hinders an atomistic description via conventional techniques (XAS, TEM) only. Here, we report the study, via multinuclear solid-state NMR and DFT modeling, of a series of Pt SACs on γ-Al 2 O 3 supports, prepared by surface organometallic chemistry followed by calcination. This approach clarifies the coordination environment of Pt 1 /γ-Al 2 O 3 , revealing that highly oxidized Pt atoms are preferentially anchored by under-coordinated Al sites at the (110) b -(100) edge. The Pt atoms have a distorted square planar or square pyramidal environment and are stabilized through [4-6] Al–O–Pt and [4] Al–OH–Pt linkages. Pyridine absorption studies reveal the presence of Brønsted acidic sites, assigned to [4] Al–OH–Pt edge moieties, through DFT modeling. The findings establish morphological features of γ-Al 2 O 3 supports needed to stabilize SACs and provide a roadmap for building accurate SAC–support models using NMR and DFT.