26 January 2022 in IEEE Transactions on Electron Devices
Identifying defects/traps is of vital importance for the implementation of high-performance Ga 2 O 3 power devices. In this work, majority and minority carrier traps in beta-gallium oxide ( $\beta $ -Ga 2 O 3 ) have been investigated and identified by means of deep level transient spectroscopy (DLTS) in Ni/ $\beta $ -Ga 2 O 3 Schottky barrier diode (SBD) and NiO/ $\beta $ -Ga 2 O 3 p + -n heterojunction diode (HJD). For both diodes, a dominant energy level of majority carrier (electron) trap states is determined to be ${E}_{C}-$ (0.75–0.79) eV with a concentration of (2.4–4.1) $\times 10^{{13}}$ cm $^{-{3}}$ . Meanwhile, an additional trapping level at ${E}_{V} +0.14$ eV with a concentration of 1.2 $\times 10^{{14}}$ cm $^{-{3}}$ yield is present in NiO/ $\beta $ -Ga 2 O 3 bipolar HJD but absent in the Ni/ $\beta $ -Ga 2 O 3 SBD unipolar counterpart. The detection of such minority carrier traps originates from the hole injection through trap-assisted tunneling (TAT) from $\text{p}^{+}$ -NiO to $\beta $ -Ga 2 O 3 . The bias- and frequency-dependent DLTS characteristics identify that such shallow-level minority carrier traps are located in the $\beta $ -Ga 2 O 3 bulk region rather not interfacial states at the NiO/ $\beta $ -Ga 2 O 3 heterointerface. The identification of both majority and minority carrier traps in this work may shed light on the in-depth understanding of carrier transport mechanisms in Ga 2 O 3 -based unipolar and bipolar power devices.
27 December 2021 in Applied Physics Letters
In this Letter, we demonstrate a large-area (1-mm2) beveled-mesa p-NiO/β-Ga2O3 bipolar heterojunction diode (HJD) with a high Baliga's figure of merit of 1.84 (2.87) GW/cm2 from DC (pulsed) measurements. Benefiting from the suppression of electric field crowing at the designed mesa edge and bipolar current conductivity modulation, the resultant device exhibits advantageous characteristics, including a low subthreshold slope of 65 mV/decade, a low DC (pulsed) differential specific on-resistance of 2.26 (1.45) mΩ cm2, a high current density of 2 kA/cm2, and a high breakdown voltage of 2.04 kV. In particular, the Ga2O3 HJD exhibits an 800 V/10 A extreme switching capability with 16.4-ns reverse recovery characteristics, as well as high operation stability at a high temperature of 200 °C. This work, thus, makes a significant step toward reaching the promise of a high figure-of-merit in β-Ga2O3 power devices.
2 March 2022 in IEEE Electron Device Letters
We report on high-performance solar-blind photodetectors fabricated on the m-plane $\alpha $ -Ga 2 O 3 epilayer grown by laser molecular beam epitaxy using the segment target approach. Benefited from the improved epitaxial quality with an $\alpha $ -(Al 0.24 Ga 0.76 ) 2 O 3 intermediate layer, the $\alpha $ -Ga 2 O 3 detector shows a low dark current of 0.23 pA, a UV/visible rejection ratio of over $10^{{5}}$ , a photo-to-dark-current ratio of ${4.4}\times {10}^{{7}}$ , a peak responsivity of 132.6 A/W, a short response time of 97 $\mu \text{s}$ , and a specific detectivity of ${1.23}\times {10}^{{15}}$ Jones at the bias of 10 V. High-temperature operation robustness is also demonstrated up to 423 K, exhibiting the reduction of dark current, a maintained high responsivity (33.9 A/W) and a speedy response (90 $\mu \text{s}$ ), which is on the frontier among the state-of-the-art Ga 2 O 3 solar-blind detectors with a record-high responsivity-bandwidth product. The temperature-dependent transient photocurrent feature implies that high gains result from the enhanced carrier lifetime due to the surface bending. It suggests that the m-plane $\alpha $ -Ga 2 O 3 detectors are promising for real-time monitoring to high-speed objectives with weak radiation flux in harsh environments.
4 October 2021 in Applied Physics Letters
In this work, we demonstrated the self-powered solar-blind photodetector based on a polyaniline/α-Ga2O3 hybrid heterojunction. The resultant device exhibited distinct self-power characteristics with a peak photoresponsivity (R) of 8.2 mA/W, a UVC (UV light of wavelength range at 200–280 nm)/UVA (UV light of wavelength range at 320–400 nm) rejection ratio (R220 nm/R400 nm) of 2.97 × 104, and a response decay time (τdec) of 176 μs at zero bias. With an elevated bias to 5 V, the dark current remained in an ultralow level of 0.21 pA, while the rejection ratio and τdec were improved to be 7.13 × 104 and 153 μs, respectively, together with the corresponding external quantum efficiency of 38.4% and a detectivity of 6.63 × 1013 Jones. Thanks to the dual functions of bandpass transmission in the deep-ultraviolet spectral region and the hole spreading transport of the polyaniline layer, the responsivity to the visible light is suppressed with the negligible internal photoemission effect, thus leading to the improved rejection ratio. Furthermore, weak interface interactions in such polyaniline/α-Ga2O3 organic–inorganic hybrid systems avoid the introduction of interfacial trapping centers by lattice mismatch and the stabilization of negatively charged anions (O2−) by (−NH2)-+species in polyaniline deactivate oxygen vacancies at the α-Ga2O3 surface, both of which lead to the negligible persistent photoconductivity effect. As a result, in the aid of the interfacial built-in field, the constructed hybrid heterojunction exhibited a self-powered detecting characteristic and a fast response speed. These findings verify the feasibility of delivering high performance photodetectors by implementing the inorganic/organic hybrid bipolar device design to overcome the difficulty in p-type Ga2O3.
17 April 2024 in Applied Physics Reviews
Impacts of spatial charge inhomogeneities on carrier transport fluctuations and premature breakdown were investigated in Schottky ampere-class Ga2O3 power diodes. Three prominent electron traps were detected in Ga2O3 epilayers by a combination of the depth-resolved capacitance spectroscopy profiling and gradual dry etching. The near-surface trap occurring at 1.06 eV below the conduction band minimum (EC), named E3, was found to be confined within a 180 nm surface region of the Ga2O3 epilayers. Two bulk traps at EC − 0.75 eV (E2*) and at EC − 0.82 eV (E2) were identified and interconnected with the VGa- and FeGa-type defects, respectively. In the framework of the impact ionization model, employing the experimental trap parameters, the TCAD simulated breakdown characteristics matched the experimental breakdown properties well, consistently with inverse proportionality to the total trap densities. In particular, the shallowest distributed E3 trap with the deepest level is responsible for higher leakage and premature breakdown. In contrast, Ga2O3 Schottky diodes without E3 trap exhibit enhanced breakdown voltages, and the leakage mechanism evolves from variable range hopping at medium reverse voltages, to the space-charge-limited conduction at high reverse biases. This work bridges the fundamental gap between spatial charge inhomogeneities and diode breakdown features, paving the way for more reliable defect engineering in high-performance Ga2O3 power devices.
28 July 2022 in The Journal of Physical Chemistry Letters