8 November 2024 in Acta Materialia
26 March 2024 in Acta Materialia
3 March 2025 in Advanced Engineering Materials
The feasibility of using recycled magnets in e‐mobility applications such as Pedelecs, e‐Scooters, and Hoverboards is being investigated with regard to their performance and recyclability. For this, a variety of end‐of‐life (EoL) magnet waste streams serve as feedstock for the production of recycled magnets which should then meet the necessary specifications for use in the above applications. After the production of a large number of such recycled magnets, these are installed in the demonstrators. Measurements on various test benches show that the demonstrators with recycled or reused magnets exhibit across the entire rotation speed range a similar or higher electromotive force or induced voltage as compared to their counterparts with primary magnets. While the e‐Scooter motor achieves almost the same induced voltage (–0.7%) by using recycled magnets, the Hoverboard motor shows even an increased voltage of 6.7%. In the case of the Pedelec motor, the reuse of EoL‐magnets leads to a voltage increase of 0.9% compared to the use of primary magnets. At the same time, an increased sustainability of these devices through a reduced CO 2 footprint can be achieved by the use of recycled or reused magnets.
21 April 2023 in Advanced Engineering Materials
Herein, the reaction behavior and chemical stability of two commercially available SmCo 2:17‐type sintered magnets with nominal composition of Sm23.75Co48.67FebalCu4.91Zr2.37 and Sm24.95Co48.80FebalCu4.46Zr2.68 (wt%) are investigated. The magnets are placed in a hydrogen atmosphere with systematically varied pressure, exposure time, and temperature ranging from 1–11 bar, 2–10 d, and 25–500 °C, respectively. Hydrogen content, magnetic properties, microstructure, and lattice constants are characterized in detail. It is found that for short exposure times like 2 d an activation temperature of 120 °C is necessary to initiate the reaction and to increase the amount of hydrogen in the Sm–Co material. Hydrogen absorption starts at lower temperatures with longer exposure times. An increase in exposure time, temperature, or pressure leads to a higher hydrogen content and a decrease in remanence Br, energy product (BH)max, and coercivity HcB. Lattice expansion, estimated by X‐ray diffraction analysis, correlates with the increasing amount of hydrogen in the Sm–Co magnets. With respect to all varied parameters under investigation, the exposure temperature has the highest impact on the observed property changes followed by reaction time and H2 pressure.
26 August 2026 in SSRN Electronic Journal
Ce substitution in Nd–Fe–B sintered magnets offers a promising pathway toward reducing the consumption of critical rare-earth elements and lowering material costs. However, the incorporation of Ce deteriorates magnetic performance due to reduced intrinsic magnetic properties and unfavourable microstructural evolution. In this work, Ce-substituted Nd–Fe–B magnets processed through the 2-powder method are systematically investigated and compared with magnets prepared by the conventional single-powder route with identical Ce contents. The 2-powder method employs a combination of a coarse Ce-containing main powder and a finer Ce-free powder to promote controlled rare-earth redistribution and shell formation during liquid-phase sintering. Magnetic properties are evaluated from room temperature up to 160 °C, while microstructural characterization is conducted across multiple length scales. The study reveals the formation of Nd/Pr-enriched shells surrounding Ce-rich grain cores, both of 2-14-1-type structure, accompanied by an optimized grain boundary phase constitution with suppressed REFe2 formation and an increased fraction of RE-rich phases. This improved grain boundary chemistry also promotes grain rearrangement during sintering, resulting in a higher degree of texture. Consequently, the 2-powder method concurrently improves the coercivity to 1054 kA m-1 and the remanence to 1.30 T with 7 wt.% Ce. These findings demonstrate that the 2-powder method provides an effective strategy for mitigating the intrinsic and metallurgical limitations associated with Ce substitution, enabling improved magnetic performance while enhancing rare-earth utilization efficiency in Nd–Fe–B permanent magnets.