Taishi Fujishiro

Taishi Fujishiro

Auto-generated profile, based on publicly available information

Taishi Fujishiro

***Nippon Steel Corporation, 20-1 Shintomi, Futtsu, Chiba, 293-8511 Japan

Research Focus & Metrics

Academic Career Length

15Years (2012-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
5 October 2022 in Corrosion
Verified
Journal Article
Closed access
PDF file
KYKyono Yasuda
Kyono Yasuda
NINobuyuki Ishikawa
Nobuyuki Ishikawa
TFTaishi Fujishiro
Taishi Fujishiro
THTakuya Hara
Takuya Hara
ETEiji Tada
Eiji Tada
MKMitsuo Kimura
Mitsuo Kimura
NACE MR0175/ISO 15156 provides the severity of a sour environment defined as a function of pH and H2S partial pressure for sulfide stress cracking. Although hydrogen-induced cracking (HIC) is also a major issue of linepipes exposed to a sour environment, the severity diagram does not necessarily correspond to the HIC susceptibility. Recently, from the viewpoint of fitness-of-purpose, the severity diagrams for HIC have been proposed based on the concept of equal hydrogen concentration. From this concept, HIC susceptibility corresponds well to the steady-state hydrogen permeability obtained from the hydrogen permeation test method. In this study, in order to clarify the relationship between HIC susceptibility and hydrogen diffusion behavior, in situ crack inspection during the HIC test and finite element method analysis of hydrogen diffusion were performed. The in situ inspection technique using phased-array ultrasonic testing which can capture the time dependence of crack distribution, and HIC initiation and propagation behaviors were clearly visualized and investigated. It was found that crack initiation and propagation stabilize as hydrogen concentration reaches a steady-state value throughout the specimen and the result was considered evidence that the HIC susceptibility corresponded with the steady value of hydrogen permeability.

24 September 2012
Verified
Conference Paper
Closed access
PDF file
TFTaishi Fujishiro
Taishi Fujishiro
THTakuya Hara
Takuya Hara
SAShuji Aihara
Shuji Aihara
Demand for natural gas using LNG and pipelines to supply the world’s gas markets is increasing. Under the large demand for high-strength linepipe, crack arrestability is one of the most important properties. DWTT (Drop Weight Tear Test) is the major test method for evaluating crack arrestability. Generally, a DWTT shear area of 85% or higher is required as the acceptance criteria, such as those of the API (American Petroleum Institute). In high-toughness linepipe steels, the abnormal fracture frequently occurs in DWTT. Abnormal fracture is defined as a cleavage fracture on the hammer side. However, the mechanism for occurrence of the abnormal fracture during DWTT has not been fully clarified. This paper describes the effect of plastic deformation on occurrence of abnormal fracture during DWTT using various steels with different microstructures. Each DWTT was carried out at the same test temperature using 20 mm plates with approximately the same tensile strength. This paper describes the deformation during DWTT, which consists of deformation caused by hammer impact, bending compression, and bending tension. The deformation due to the impact of the hammer during DWTT on a 20 mm plate was limited, and the location affected by the hammer impact did not correspond to that where abnormal fracture occurred. Moreover, the equivalent plastic strain from bending deformation was dominant as compared with that of hammer impact regardless of the microstructure. This suggests that abnormal fracture occurred by exceeding the critical equivalent plastic strain due to the bending deformation.