Integration of β-Ga2O3 with high thermal conductivity materials such as diamond has been considered due to β-Ga2O3's low and anisotropic thermal conductivity, reaching only 27 W m–1 K–1. However, the effect of crystallographic orientation on thermal interface resistance has not been studied extensively, which is relevant for potential device architectures. In this work, we use molecular dynamics simulations to investigate the crystal orientation-dependent thermal boundary resistance (TBR) across van der Waals bonded diamond–β-Ga2O3 and ionicly bonded amorphous Al2O3–β-Ga2O3 interfaces. Al2O3 is often used as interlayer to grow diamond onto Ga2O3. We find that TBR values across the van der Waals interface may vary by up to 70% depending on the orientation of the β-Ga2O3, while the Al2O3–β-Ga2O3 TBR values remain around 0.9 ± 0.3 m2 KGW−1. We, thus, conclude on the optimal direction of β-Ga2O3 to use for reducing the TBR in these heterostructures.
10 September 2021 in IEEE Transactions on Electron Devices
The design space of Ga 2 O 3 -based devices is severely constrained due to its low thermal conductivity and absence of viable p-type dopants. In this work, we discuss the limits of operation of a novel Ga 2 O 3 –Al 2 O 3 –diamond-based super-junction device concept, which can alleviate the constraints associated with Ga 2 O 3 -based devices. The improvements achieved using the proposed device concept are demonstrated through electrical and thermal simulations of Ga 2 O 3 –Al 2 O 3 –diamond-based super-junction Schottky barrier diodes (SJ-SBDs) and non-punch-through or conventional Schottky barrier diodes (NP-SBDs). The SJ-SBD enables operation below the ${R}_{\mathrm {\scriptscriptstyle ON}}$ -breakdown voltage limit of Ga 2 O 3 NP-SBD, enabling >4 kV blocking voltage at ${R}_{\mathrm {\scriptscriptstyle ON}}$ of 1–3 $\text{m}\Omega $ cm 2 . The maximum switching frequency of SJ-SBD may be only a few kHz, as it is limited by the activation energy of acceptors (0.39 eV) in the diamond. Crucially, compared with NP-SBD, the use of diamond also results in ~60% reduction in temperature rise during static power dissipation. Polycrystalline diamond (PCD) properties depend on detailed microstructure and benefits compared to ideal Ga 2 O 3 NP-SBD arise for diamond critical fields ≥6 MV/cm and thermal conductivities as low as 50–150 W/(m $\cdot $ K).
Metal-semiconductor interface is a bottleneck for the efficient transport of charge carriers through transition metal dichalcogenide (TMD)-based FETs. Injection of charge carriers across such interfaces is mostly limited by the Schottky barrier at the contacts that must be reduced to achieve highly efficient contacts for carrier injection into the channel. Here, we introduce a universal approach involving dry chemistry to enhance atomic orbital interaction among various TMDs (Mo₂, W₂, MoSe₂, and WSe₂) and metal contacts. Quantum chemistry among TMDs, chalcogens, and metals has been explored using detailed atomistic (DFT and NEGF) simulations, which is then verified using Raman, PL, and XPS investigations. Atomistic investigations revealed lower contact resistance due to the enhanced orbital interaction and unique physics of charge sharing between constituent atoms in TMDs with the introduced chalcogen atoms that are subsequently validated through experiments. In addition to contact engineering, which resulted in contact resistance (extracted via the Y-function method as low as 119 and 59 Ωμm in Mo₂ and W₂, respectively), a novel approach to cure/passivate the dangling bonds present at the 2-D TMD channel surface has been demonstrated. While the contact engineering improved the ON-state performance (ION, gm, μ, and RON) of the 2-D TMD FETs by orders of magnitude, chalcogen-based channel passivation was found to improve gate control (IOFF, SS, and VTH) significantly. This resulted in an overall performance boost. The engineered TMD FETs were shown to have performance on par with the best reported until now.
Developing future electronics will require aggressive scaling of the channel material thickness while maintaining device performance. Two-dimensional (2D) semiconductors are promising candidates to sustain further device scaling, but despite more than two decades of intense research, experimental performance continues to lag theoretical expectations. Here, we develop an oxygen-free approach to fabricate 2D field-effect transistors and push the electrical transport toward the theoretical phonon-limited intrinsic mobility. This approach achieves record carrier mobilities of 91 and 132 cm2 V-1 s-1 for mono- and bilayer MoS2 transistors on silicon oxide substrates. Statistical analysis of over 60 MoS2 and WS2 devices confirms that oxygen-free fabrication enhances device performance by more than an order of magnitude across key figures of merit. While previous studies suggest that 2D transition metal dichalcogenides such as MoS2 and WS2 are relatively stable in air, we show that even short-term ambient exposure can degrade their performance. We identify oxygen as a crucial factor in limiting transistor performance through irreversible chemisorption. This study emphasizes the criticality of avoiding oxygen exposure and offers guidance for device manufacturing that impacts fundamental research and practical applications of 2D materials.
A ledge feature in the capacitance–voltage (CV) profiles of Ga2O3 MOS (metal–oxide–semiconductor) capacitors is investigated using UV-assisted CV measurements. A model is presented whereby the capacitance ledge is associated with carrier trapping in deep-level states at the Al2O3/Ga2O3 interface. Following UV assisted emptying of interface traps at a constant bias, a voltage ramp toward flatband results in a CV ledge when the trap recombination current becomes equal to the quasi-static sweep charging current. The ledge continues until all the traps below the corresponding pinned surface potential have been filled. Varying the UV energy varies the ledge voltage range and allows a density of states to be determined as a function of energy. A broad interface state peak with maximum density ∼8 × 1012 cm−2 eV−1 for deep trap energies lying between 2.4 and 4.1 eV below the conduction band (CB) edge is extracted. Using the conductance method, the interface trap density is also found to rise toward the CB edge in the range 0.25–0.45 eV below the CB edge, reaching a maximum density of ∼1 × 1012 cm−2 eV−1. Combining these two techniques, an interface trap distribution is estimated for almost the entirety of the bandgap of Ga2O3. This novel technique probes deep interface states where standard methods fail to quantify interface states reliably.