7 October 2020 in Nanotechnology
We report the crystal structures of GaAs and GaAs/GaNAs/GaAs core–multishell nanowires (NWs). From statistical investigations by x-ray diffraction (XRD) and electron backscattered diffraction (EBSD) pattern analysis, we statistically and microscopically resolve the zinc-blende (ZB) and wurtzite (WZ) polytypism within the NWs. The XRD analysis shows a smaller fraction of WZ segments in the NWs with a larger concentration of nitrogen. With increasing nitrogen content in the GaNAs shell, the ZB peak position shifts toward higher angles and the WZ peak intensity decreases. The EBSD measurements also confirm the coexistence of ZB and WZ polytypes in all of the NWs. Their polytype switches along the length. Twin defects are observed in the ZB segments in all of the NWs. The unique grain map and grain size distribution show a decrease of the WZ segments in the GaAs/GaNAs/GaAs NW, in agreement with the XRD results. Microscopically, the local area where the polytype switches from WZ in the inner-core side to ZB toward the outer-shell surface is observed. Overall, we propose that the WZ polytype in the GaAs NWs decreases because of the strain induced by the growth of the GaNAs shell with a smaller lattice constant.
21 August 2023 in Applied Physics Letters
Semiconducting nanowires (NWs) fabricated from III–V materials have gained significant attention for their application in advanced optoelectronic devices. Here, the growth of GaAs/GaInNAs/GaAs core-multishell NWs with a triple quantum-well structure, having about 2% N and 20% In, is reported. The NWs are grown via selective area plasma-assisted molecular beam epitaxy on patterned Si(111) substrates with SiO2 mask holes. The nucleation and growth of the GaAs nanowires' core are carried out by Ga-induced vapor–liquid–solid growth at the open holes. Finely controlled, vertically aligned, regular core-multishell NWs with uniform wire length and diameter are obtained with a 96% yield and targeted nitrogen concentrations of 0%, 2%, and 3%. The GaInNAs NWs exhibit a spectral red shift relative to the GaAs NWs' peak. Their emission wavelength increases with the N content reaching up to 1.26 μm, which makes them a promising tool in telecommunication light sources.