The influence has been studied of thermo-mechanical treatment, sensitization conditions, and neutron irradiation on the pitting corrosion resistance of austenitic 316LN stainless steel variants in 10% FeCl3·6H2O at 22 °C. Variants of this steel were modified with additions of nitrogen, manganese, copper, and tungsten, as well as testing cast, cold-rolled, grain boundary engineered (GBE), and as-received variants. It was found that the 316LN steel variant with additions of 0.2% N and 2% Mn had the best pitting corrosion resistance of all studied conditions. When irradiated in a light water reactor (LWR) to a maximum fluence of 3 × 1017 n/cm2 (E > 1.1 meV, Tirr < 50 °C), neutron irradiation surprisingly increased the resistance of GBE steels to pitting corrosion. An anisotropy of corrosion resistance of GBE and cold rolled steels was observed.
The paper studies the features of martensitic transformation during plastic deformation (uniaxial tension and compression) of austenitic steels 12X18N10T and AISI304 irradiated with thermal neutrons to a fluence of 3.7·1020 n/cm2 . The nickel equivalent and stacking fault energy values for 12X18N10T and AISI304 steels are calculated. It is established that AISI304 steel is more prone to martensitic transformation. The mechanical characteristics of the studied steels under uniaxial tension are determined. It is shown that with similar strength characteristics, the plasticity of irradiated AISI304 steel is twice as high as that of 12X18N10T steel. This fact is due to the more intense martensitic transformation during the plastic deformation of AISI304 steel.
The article is devoted to the study of the resistance of structural materials of the BN-350 reactor to pitting corrosion in an aqueous medium containing chlorine ions in the presence of organic corrosion inhibitors. The results of accelerated testing of samples of austenitic steels 12Cr18Ni10Ti, 08Cr16Ni11Mo3Ti and Cr13Mo2NbVB (EP-450) ferrite-martensitic steel for pitting corrosion in a 10% aqueous solution of iron three-chloride hexahydrate without an inhibitor and in the presence of various concentrations of corrosion inhibitor are presented. The effect of heat treatment on the pitting resistance of structural steels is studied and the role of carbide precipitates of MC and M23C6 types in pitting defects formation is discussed.