A series (10 examples) of thienyl spacing D–π-A push–pull chromophores end-capped with a triphenylamine (TPA) donor and tetracyanobutadiene (TCBD) acceptor have been synthesized in high yields. The synthesis of these chromophores as well as their synthetic precursors was accomplished in good to excellent chemical yields. Interestingly, acetylenic precursors displayed strong emissive properties with a large Stokes shift and positive solvatochromism behaviour. The photophysical investigation of the targeted chromophores revealed that their low optical band gap (ca. 1.38 to 1.62 eV) coupled with excellent molar absorptivity (ca. 28 800 to 90 500 M−1 cm−1) ensures good light-harvesting properties, while the electrochemical studies revealed their deep HOMO (ca. −5.31 to −5.16 eV) and LUMO (ca. −3.49 to −4.31 eV) energy levels suggesting them to be promising semiconducting materials for organic solar cell applications. An inverse bulk heterojunction (BHJ) photovoltaic device with a cell configuration of ITO/ZnO/BHJ/V2O5/Ag was fabricated to demonstrate the potential applications of these molecular semiconductors as active layer materials. A cursory analysis of the device performance of all materials under identical conditions showed a reasonable power conversion efficiency ranging from 1.95 to 3.33%. These initial results are encouraging for TPA-TCBD adjoined semiconductors with an indication of prospective applications and development, since their potential was little explored in small molecule-based organic solar cells.
9 January 2024 in Colloids and Surfaces A: Physicochemical and Engineering Aspects
Cross-linked polymer (CLP) composed of poly(ethylene glycol) methyl ether acrylate and poly(ethylene glycol) diacrylate has been used in synthesizing gel electrolyte. A set of electrolyte samples was synthesized using gel casting method by varying the weight percentage ratio of cross-linked polymers from 2–14 % in an incremental order (2 %) with respect to poly (ethylene oxide) (PEO) and evaluated its performance by employing in the fabrication of dye-sensitized solar cells. The synthesized polymer was subjected to different analytical techniques such as NMR, TGA, DSC, GPC, and FTIR to confirm the materials. The molecular weight of the CLP has been measured using GPC and the obtained value is found to be 3.655 KDa with polydispersity of 1.94. The CLP-PEO gel electrolyte with 10 % weight ratio has obtained the highest ionic conductivity of 3.07 × 10−6 S/cm−1 at room temperature and best photo-conversion efficiency of 5.1 % was achieved for the same.