Mn and Cu doped ZnS nanoparticles in powder form were prepared by a simple solvothermal route. Particle size and crystal structure of the products were investigated through X-ray diffraction study revealing the formation of cubic ZnS nanoparticles of average diameter 2.5 nm. Particle size was also verified by the high resolution transmission electron microscopic images. Blue emission at ∼445 nm was observed from the undoped sample, which was attributed to the presence of large surface defects. With increasing doping concentration the defect related emission gradually quenches and subsequently the impurity related emissions appeared. Mn doped samples exhibited orange emission at ∼580 nm which may be attributed to the transition between 4T1 and 6A1 energy levels of the Mn2+ 3d states. Whereas, the Cu doped ZnS nanoparticles exhibited a red shifted strong blue emission at ∼466 nm which is attributed to the transition of the electrons from the surface states to the 't2' levels of Cu impurities.
1 February 2007 in Journal of Nanoscience and Nanotechnology
CdS nanorods with varying dimensions were synthesized by solvothermal process. It was observed that the anions present with the Cd-salts play an important role in determining the dimensions of the CdS nanorods. The crystalline nature of the sources was found to play a crucial role in determining the phase of the products. The nature of the sulfur source, molar ratio of the precursors, filling fraction of the solvent, and the synthesis temperature play important role in defining the size and shape of the products. By controlling the experimental parameters it was possible to control the dimension of the CdS nanorods within a certain range (diameter of the nanorods could be varied within a wide range from ∼7 to 100 nm by varying the temperature within 100–250 °C). Optical absorption, photoluminescence, and Raman studies of these samples were carried out to characterize the CdS nanorods.
We present the electronic transport characteristics of ternary alloy Cd(1-x)Zn(x)S nanowire networks in the dark and under white light illumination. Compared to the negligible dark current, we observed a photocurrent enhancement of up to four orders of magnitude at an intensity of 460 mW cm(-2). The time constant of the dynamic photoresponse is approximately 5 s. The current-voltage characteristics at different intensities show Ohmic behavior at low bias and space charge limited conduction (SCLC) at higher bias voltages. The SCLC behavior and slow time response indicate that the charge transport is dominated by tunneling at the percolating inter-nanowire junctions.