23 January 2023 in Acta Materialia
1 October 2019 in Materials Letters
1 March 2024 in Materialia
24 September 2023 in Advanced Engineering Materials
4 April 2024 in Materials Letters
1 January 2022 in SSRN Electronic Journal
Cr-rich αʹ precipitation during aging typically leads to hardening and accordingly embrittlement of FeCrAl alloys, which needs to be suppressed. The influence of grain size on αʹprecipitation was studied by aging coarse-grained (CG), ultra-fine grained(UFG), and nanocrystalline (NC) ferritic Kanthal-D [KD; Fe-21Cr-5Al (wt.%) alloy] at 450, 500 and 550oC for 500h. After aging at 450 and 500oC, less hardening was observed in the UFG KD than in CGKD. Atom probe tomography indicated a lower number density and larger sized αʹ in the fine-grained versus the CG alloys. The smaller grain size and higher defect (vacancy and dislocation) density in the UFG KD facilitated diffusion and accordingly enhanced precipitation kinetics, leading to coarsening of precipitates, as well as saturation of precipitation at lower temperatures, as compared to those in CG KD. No hardening occurred in UFG and CG KD after aging at 550oC, indicating that the miscibility gap is between 500 and 550oC. NC KD exhibited softening after aging owing to grain growth. αʹprecipitation occurred in NC KD aged at 450oC but not at 500oC, indicating that miscibility gap is between 450 and 500oC. Thus, the significantly smaller grain size in NC KD decreased the miscibility gap, as compared to that in CG and UFG KD. This is attributed to the absorption of vacancies by migrating grain boundaries during aging, suppressing αʹ nucleation and enhancing Cr solubility.