1 April 2002 in Applied Optics
The influence on the internal stress and optical properties of Nb2O5 thin films with ion-beam energy was investigated. Nb2O5 thin films were deposited on unheated glass substrates by means of ion-beam sputtering with different ion-beam voltage, V b. The refractive index, extinction coefficient, and surface roughness were found to depend on the ion-beam energy. The stresses in thin films were measured by the phase-shifting interferometry technique. The film stress was also found to be related to V b, and a high compressive stress of -0.467 GPa was measured at V b = 850 V. The Nb2O5–SiO2 multilayer coatings had smaller average compressive stress as compared with single-layer Nb2O5 film.
9 February 2009 in Applied Physics Letters
Wide-band gap ZnO semiconductors are attractive materials for the investigation of microcavity exciton polaritons due to the large exciton binding energy and oscillator strength. We report the growth and characterization of bulk ZnO-based hybrid microcavity. The phenomenon of strong exciton-photon coupling at room temperature has been observed in the ZnO-based hybrid microcavity structure, which consists of 30 pair epitaxially grown AlN/AlGaN distributed Bragg reflector (DBR) on the bottom side of the thick ZnO cavity and 9 pair DBR as the top mirror. The cavity quality factor is about 221. The experimental results show good agreement with theoretically calculated exciton-polariton dispersion curves based on transfer matrix method. From the theoretical and experimental exciton-polariton dispersion curves with two different cavity-exciton detuning values, the large vacuum Rabi splitting is estimated to be about 58 meV in the ZnO-based hybrid microcavity.
1 March 2006 in Applied Optics
Composite films of oxide with refractive indices that varied from 1.48 to 2.15 were realized by using rf ion-beam sputtering. All the composite films were amorphous and had a surface roughness of less than . The inhomogeneity of the composite was discussed, and a rugate filter was designed and fabricated by automatic computer control.
20 May 2005 in Applied Optics
The effects of thermal annealing of titanium oxide films deposited by ion-beam assistance at annealing temperatures from 100 °C to 300 °C on the residual stress and optical properties of the films was investigated. The refractive indices and extinction coefficients increased gradually as the temperature was increased from 100 °C to 200 °C and then declined gradually as the temperature was increased further from 200 °C to 300 °C. The film lost oxygen and slowly generated lower suboxides as the annealing temperature was reduced below 200 °C, as determined by x-ray photoelectron spectroscopy (XPS). As the annealing temperature increased above 200 °C, the lower suboxides began to capture oxygen and form stable oxides. XPS measurements were made to verify both the binding energy associated with the Ti 2p line and the variation of the O 1s line. A Twyman–Green interferometer was employed for phase-shift interferometry to study the residual stress. The residual stress declined as the temperature was reduced from 100 °C to 200 °C because the lower suboxides reduced the stress in the film. Above 200 °C, the film began to capture oxygen, so the residual stress rose. At 300 °C, the film was no longer amorphous as the anatase was observed by x-ray diffraction.
1 December 2005 in Applied Optics
Aluminum fluoride (AlF3) was deposited by a resistive heating boat. To obtain a low optical loss and high laser-induced damage threshold (LIDT) at 193 nm, the films were investigated under different substrate temperatures, deposition rates, and annealing after coating. The optical property (the transmittance, refractive index, extinction coefficient, and optical loss) at 193 nm, microstructure (the cross-sectional morphology, surface roughness, and crystalline structure), mechanical property (stress), and LIDT of AlF3 thin films have been studied. AlF3 thin films deposited at a high substrate temperature and low deposition rate showed a lower optical loss. The highest LIDT occurred at the substrate temperature of 150 °C. The LIDT of the films prepared at a deposition rate of 2 Å/s was higher than that at other deposition rates. The annealing process did not influence the optical properties too much, but it did increase the LIDT and stress.
1 July 2005 in Thin Solid Films