We have studied the correlation between the elastocaloric effect and the crystallographic direction where a uniaxial stress is applied in a textured polycrystalline Ni-Mn-In-Cr ferromagnetic shape memory alloy; this alloy displays martensitic transformation around room temperature and presents an L21 cubic structure in the austenite phase. The texture in the material was induced by simple arc melting synthesis; using inverse pole figures, a favored grain growth was shown in the direction [001] perpendicular to the cooled surface. The elastocaloric effect was determined by direct measurements of the adiabatic temperature change (ΔTadme), while compressive stress was applied and released; hereby, it has been shown that it is possible to exploit the columnar growth texture in order to obtain a large and reversible elastocaloric effect. The reversible elastocaloric response was measured between 280 and 310 K by applying moderate stresses of 50, 75, and 100 MPa in the [001], [111], and [011] directions. A strong interrelation was found in the cyclic ΔTadme values of −3.9, −2.0, and −1.3 K after unloading a compressive stress of 100 MPa applied mainly in the [001], [111], and [011] directions, respectively.
The investigation of caloric effects linked to first-order structural transitions in Heusler-type alloys has become a subject of considerable current interest due to their potential utilization as refrigerants in solid-state cooling devices. This study is mainly motivated by the possibility of developing refrigeration devices of improved energy efficiency with a reduced environmental impact. We produced partially textured and isotropic bulk samples of the Heusler-type magnetic shape memory alloy Ni55Fe11Mn7Ga27 by arc melting and spark plasma sintering (SPS), respectively. Their structural, microstructural, and phase transition characteristics and magnetocaloric and elastocaloric effects, associated with first-order martensitic transformation (MT), were studied. The elemental chemical compositions of both samples were close to nominal, and a martensitic-like structural transformation appeared around room temperature with similar starting and finishing structural transition temperatures. At room temperature, austenite exhibited a highly ordered L21-type crystal structure. The partial grain orientation and isotropic nature of the arc-melted and SPS samples, respectively, were revealed by X-ray diffraction and SEM observations of the microstructure. For the arc-melted sample, austenite grains preferentially grew in the (100) direction parallel to the thermal gradient during solidification. The favorable effect of the texture on the elastocaloric response was demonstrated. Finally, due to its partial grain orientation, the arc-melted bulk sample showed superior values of maximum magnetic entropy change (|ΔSM|max = 18.6 Jkg−1K−1 at 5 T) and elastocaloric adiabatic temperature change (|ΔTadme|max = 2.4 K at 120 MPa) to those measured for the SPS sample (|ΔSM|max = 8.5 Jkg−1K−1 and (|ΔTadme|max = 0.8 K).
Tantalum (Ta) is an excellent alternative for structural orthopedic implants because of its high biocompatibility and chemical stability, but its melting point of 3020 °C severely complicates conventional casting. To address this, the study evaluates spark plasma sintering (SPS) to consolidate pure Ta powders at 1450 °C and 50 MPa and analyzes the impact of heating rates (50–200 °C/min) on microstructural, mechanical, wear, and corrosion properties. Results indicate that heating rate dictates final densification: a 50 °C/min rate achieved 98.59% relative density, whereas 200 °C/min yielded only 82.28% due to reduced thermal exposure. Sintering involved dislocation creep and viscous flow mechanisms, with X-ray diffraction confirming a stable α-Ta matrix across all samples. Mechanically, the 50 °C/min samples achieved a maximum microhardness of 285 HV, whereas higher porosity at 200 °C/min reduced hardness by 27.8%. Wear testing showed a two-stage friction evolution: an initial Ta2O5 solid-lubricating effect, followed by predominant abrasion and adhesion, with stable wear rates (3.2 to 3.6 × 10−3 mm3/N·m) for dense specimens. Finally, tests in simulated body fluid confirmed spontaneous self-passivation. However, the corrosion rate increased with heating rates, indicating that the resulting porosity adversely affects the material’s surface response.