In this paper, five grading functional gradient lattice structures with a different density perpendicular to the loading direction were proposed, and the surface morphology, deformation behavior, and compression properties of the functional gradient lattice structures prepared by selective laser melting (SLM) with Ti-6Al-4V as the building material were investigated. The results show that the characteristics of the laser energy distribution of the SLM molding process make the spherical metal powder adhere to the surface of the lattice structure struts, resulting in the actual relative density of the lattice structure being higher than the designed theoretical relative density, but the maximum error does not exceed 3.33%. With the same relative density, all lattice structures with density gradients perpendicular to the loading direction have better mechanical properties than the uniform lattice structure, in particular, the elastic modulus of LF, the yield strength of LINEAR, and the first maximum compression strength of INDEX are 28.99%, 16.77%, and 14.46% higher than that of the UNIFORM. In addition, the energy absorption per unit volume of the INDEX and LINEAR is 38.38% and 48.29% higher, respectively, than that of the UNIFORM. Fracture morphology analysis shows that the fracture morphology of these lattice structures shows dimples and smooth planes, indicating that the lattice structure exhibits a mixed brittle and ductile failure mechanism under compressive loading. Finite element analysis results show that when the loading direction is perpendicular to the density gradient-forming direction, the higher density part of the lattice structure is the main bearing part, and the greater the density difference between the two ends of the lattice structure, the greater the elastic modulus.
3 August 2024 in Journal of Manufacturing Processes
Using finite element analysis software and based on the Johnson–Cook failure criterion, a 3D printing workspace model with collapse, powder sticking, and cavity defects was established under the selective laser melting (SLM) forming process. The simulation analysis of milling holes was carried out, and the relationship between cutting speed and material-removal rate on tool wear and entrance burr was derived. The hole-milling experiment was carried out to verify the dimensional accuracy and surface appearance of the hole under the two processes of SLM direct forming and re-milling after forming; the inhibition effect of re-milling after forming on collapse, powder sticking, and cavity defects in hole forming were studied, and the formation mechanism of various defects such as burrs, scratches, and hole-wall cracks in the hole-milling process was analyzed. The Kistler9129A dynamometer was used to measure the cutting forces of re-milling holes and direct milling holes, and a comparative analysis was carried out. The influence of cutting speed, hole diameter, and material-removal rate on the axial force of milling holes was explored. The experiment results were consistent with the simulation cutting model, and the model’s accuracy was verified.
This paper presents an in-depth study of the variable reference process to improve the organization and properties of selective laser melting TC4 specimens. A relationship equation between body energy density and stratification is proposed. This study aimed to look into how layer and volume energy density affect the surface, tensile characteristics, and microstructure of specimens. The test findings demonstrated that specimen densities rise as the power index falls, with the most excellent density reaching 99.42%. The number of secondary α’ phases declined as the energy density of the laminae slowed down. The tensile strength of these specimens reached 1190.84 MPa, and the yield strength came at 1103.87 MPa with the same interval of variable laser power. This offers a fresh avenue for research into SLM to enhance the specimens’ overall performance.