We have investigated the effects of deposition temperature and post-annealing on the passivation performance of AlOx films deposited by O3-based atomic layer deposition for crystalline Si. We found that the dramatic enhancement in the passivation performance of room-temperature deposited AlOx films by post-annealing is due to the phase transformation of aluminum silicate to mullite in an AlOx interlayer and the resulting self-aligned AlOx/SiOx interface. This result is interesting for the fabrication of high-performance silicon solar cells with AlOx passivation layers.
Although crystalline silicon is widely used as substrate material for solar cell, many defects occur during crystal growth. In this study, the generation of crystalline defects in silicon substrates was evaluated. The distributions of small-angle grain boundaries were observed in substrates sliced parallel to the growth direction. Many precipitates consisting of light elemental impurities and small-angle grain boundaries were confirmed to propagate. The precipitates mainly consisted of Si, C, and N atoms. The small-angle grain boundaries were distributed after the precipitation density increased. Then, precipitates appeared at the small-angle grain boundaries. We consider that the origin of the small-angle grain boundaries was lattice mismatch and/or strain caused by the high-density precipitation.
10 September 2023 in Solar Energy Materials and Solar Cells
This research investigates the carrier recombination properties of a crystalline defect layer introduced by the plasma enhanced chemical vapor deposition (PECVD) process of amorphous hydrogenated silicon nitride (SiNx) passivation films. A direct PECVD technique was used for SiNx films deposition. A crystalline defect layer existed on the surface of the silicon substrate and is under the SiNx passivation film. The recombination lifetime in this defect layer was obtained by focusing on the thickness of the defect layer and the effective lifetime before and after the defect layer etching. After etching a few nanometer thickness, effective lifetime drastically increased. On the other hands, the carrier recombination center could be electrically inactivated by 600°C annealing after SiNx deposition. According to the depth profile of effective lifetime, it was clarified the high carrier recombination region were concentrated near the surface of silicon substrate.
21 December 2009 in Japanese Journal of Applied Physics