In this paper, potassium salt roasting additives were applied to extract vanadium from vanadium–titanium magnetite concentrate. Meanwhile, the mechanisms of potassium salt roasting and acid leaching kinetics were investigated. The results indicate that potassium salt roasting additives are more efficient than sodium and calcium salt and that K2SO4 works best. Under certain conditions (a dosage of K2SO4 of 4 wt %, a roasting temperature of 900 °C, a roasting time of 1 h, a leaching temperature of 95 °C, a sulfuric acid concentration of 10% (v/v), and a leaching time of 1.5 h with a liquid to solid ratio of 3 mL/g) the vanadium leaching efficiency reached 71.37%, an increase of 30.20% compared to that of blank roasting. Additionally, XRD and related SEM-EDS analyses indicated that K2SO4 fully destroyed the structure of vanadium-bearing minerals such as magnetite, and promoted the generation of soluble KVO3 to inhibit the formation of insoluble Ca(VO3)2 in the roasting process. Furthermore, it promoted the dissolution of sphene and the release of its vanadium in the leaching process, which increased the vanadium leaching efficiency significantly. Meanwhile, leaching kinetics analyses showed that the leaching process was controlled by internal diffusion; the apparent activation energy decreased from 37.43 kJ/mol with blank roasting to 26.31 kJ/mol with potassium salt roasting. The reaction order, with regards to the sulfuric acid concentration, decreased from 0.6588 to 0.5799. Therefore, potassium salt roasting could improve mineral activity, accelerating the leaching process and reducing the dependence on high temperature and high acidity.
This study investigated bioleaching behavior of vanadium from a vanadium-bearing shale using Acidithiobacillus ferrooxidans (A. ferrooxidans). Results showed a maximum recovery of 62% vanadium in 1.2-day bioleaching, which was 22.45% higher than the controls. Then, the vanadium leaching efficiency decreased significantly, only 24% of that was obtained on the tenth day. The vanadium extraction in 1.2 days was mainly attributed to the dissolution of vanadium in free oxides of shale. Fe3+ produced by A. ferrooxidans promoted the dissolution process. X-ray diffraction (XRD) patterns of the leached residues confirmed the generation of jarosite. SEM-EDS analysis of the residues indicated that jarosite adsorbed on the shale and inhibited the further dissolution of vanadium. The relevance of V, Fe, S, O was quite good in the energy disperse X-ray spectrometry (EDS) element mapping of jarosite, and acid-washing of the jarosite resulted in 31.6% of the vanadium in the precipitates desorption, indicating that the decrease of vanadium leaching efficiency in bioleaching process was caused by both adsorption and co-precipitation with jarosite.