High-strength concrete (HSC) provided significant advances in civil construction due to its superior strength, efficiency, and durability against environmental attacks. However, given the high cement content, low water-to-cement ratio, and the presence of mineral additives, it is crucial to prevent the development of induced tensile stresses that can lead to autogenous shrinkage. This shrinkage may result in cracking of structural elements, thereby compromising durability. One method explored to reduce autogenous shrinkage in HSC is the use of superabsorbent polymers (SAP) as internal curing agents. In this context, this work aims to analyze the influence addition of SAP and nano silica (NS) on the durability of Portland cement microconcrete. For this, the experimental program consisted of three mixtures of high-strength microconcrete: one containing 0.3% SAP, another containing 0.3% SAP and 1% NS, and one used as a reference with a water/cement ratio equal to 0.35. The behavior of concrete in its hardened state was assessed through the execution of the following tests: simple axial compression strength, modulus of elasticity, water absorption by capillarity and immersion, electrical resistivity, and chloride migration. The results indicate that incorporating SAP does not lead to a reduction in the mechanical properties or durability of the microconcretes; instead, it enhances these properties. Additionally, while the addition of NS causes a negligible increase in modulus and strength values at 28 days, it significantly boosts compressive strength at earlier ages. The microconcrete containing SAP and NS showed the best performance in the durability tests, indicating that the addition of NS further enhanced the concrete's durability. It was confirmed that the dense microstructure typical of HSC is maintained even with the presence of pores formed by the SAP desorption process. This is because these pores are larger and isolated, rather than smaller and interconnected.