12 December 2021 in Materials
Verified
Journal Article
Open access
PDF file
YCYuliia Chabak
Yuliia Chabak
BEBohdan Efremenko
Bohdan Efremenko
IPIvan Petrišinec
Ivan Petrišinec
VEVasily Efremenko
Vasily Efremenko
Angeliki G. LekatouAngeliki G. Lekatou
Angeliki G. Lekatou
TPTatiana Pastukhova
Tatiana Pastukhova
The structural features and nanoindentation/tribological properties of 316 stainless steel fabricated by conventional rolling and laser-based powder bed fusion (LPBF) were comparatively investigated regarding the effect of surface-pulsed plasma treatment (PPT). PPT was performed using an electrothermal axial plasma accelerator under a discharge voltage of 4.5 kV and a pulse duration of 1 ms. Optical microscopy, scanning electron microscopy, X-ray diffraction, nanoindentation measurements and tribological tests were applied to characterize the alloys. The LPBF steel presented almost the same modulus of elasticity and double the hardness of rolled steel. However, the LPBF steel manifested lower dry-sliding wear resistance compared with its wrought counterpart due to its porous structure and non-metallic inclusions. Conversely, LPBF steel showed three times higher wear resistance under sliding in simulated body fluid (SBF), as compared with wrought steel. PPT led to steel modification through surface melting to a depth of 22–26 μm, which resulted in a fine cellular structure. PPT moderately improved the dry-sliding wear resistance of LPBF steel by fusion of pores on its surface. On the other hand, PPT had almost no effect on the SBF-sliding wear response of the steel. The modification features were analyzed using a computer simulation of plasma-induced heating.

1 January 2017 in Journal of Friction and Wear
Verified
Journal Article
Closed access
PDF file
VEV. G. Efremenko
V. G. Efremenko
KSK. Shimizu
K. Shimizu
TPT. V. Pastukhova
T. V. Pastukhova
YCYu. G. Chabak
Yu. G. Chabak
KKK. Kusumoto
K. Kusumoto
VEVasily Efremenko
Vasily Efremenko
The results of an investigation of the effect of bulk quenching from temperature in the range of 760–1050°C, cryogenic treatment (–196°C) and surface plasma hardening on the abrasive-erosion wear of...

3 June 2016 in International Journal of Minerals, Metallurgy and Materials
Verified
Journal Article
Closed access
PDF file
VEVasily Efremenko
Vasily Efremenko
KSK. Shimizu
K. Shimizu
ACA. P. Cheiliakh
A. P. Cheiliakh
TPT. V. Pastukhova
T. V. Pastukhova
YCYu. G. Chabak
Yu. G. Chabak
KKK. Kusumoto
K. Kusumoto

29 January 2018 in International Journal of Materials Research
Verified
Journal Article
Closed access
VEVasily Efremenko
Vasily Efremenko
KSKazumichi Shimizu
Kazumichi Shimizu
TPTatiana Pastukhova
Tatiana Pastukhova
YCYuliia Chabak
Yuliia Chabak
MBMichail Brykov
Michail Brykov
AEAlexey Efremenko
Alexey Efremenko
The effect of heat treatment and chromium contents (up to 9.1 wt.%) on the wear resistance of spheroidal carbide cast iron (9.5 wt.% V) was studied using optical and scanning electron microscopy, X-ray diffractometry, dilatometry and three-body abrasive testing. It was found that quenching from 760 °C and 920 °C improved the alloys’ wear resistance compared to the as-cast state due to the formation of metastable austenite transforming into martensite under abrasion. The wear characteristics of alloys studied are 1.6 – 2.3 times higher than that of reference cast iron (12 wt.% V) having stable austenitic matrix. Chromium addition decreases surface damage due to the formation of M 7C3 carbides, while it reduces wear resistance owing to austenite stabilization to abrasion-induced martensite transformation. The superposition of these factors results in decreasing the alloys’ wear behaviour with chromium content increase.

1 March 2020 in Journal of Friction and Wear
Verified
Journal Article
Closed access
PDF file
VZVadym Zurnadzhy
Vadym Zurnadzhy
VEVasily Efremenko
Vasily Efremenko
MBM. N. Brykov
M. N. Brykov
IPI. Petryshynets
I. Petryshynets
TPT. V. Pastukhova
T. V. Pastukhova
RKR. A. Kussa
R. A. Kussa
This article presents the results of a study of the effects of the amount and metastability of retained austenite on the abrasive wear resistance of 0.55%

19 June 2021 in Materials
Verified
Journal Article
Open access
PDF file
YCYuliia Chabak
Yuliia Chabak
VEVasily Efremenko
Vasily Efremenko
MDMiroslav Džupon
Miroslav Džupon
SKShimizu Kazumichi
Shimizu Kazumichi
VFViktor Fedun
Viktor Fedun
TPTatiana Pastukhova
Tatiana Pastukhova
The structural and tribological properties of a protective high-chromium coating synthesized on gray cast iron by air pulse-plasma treatments were investigated. The coating was fabricated in an electrothermal axial plasma accelerator equipped with an expandable cathode made of white cast iron (2.3 wt.% C–27.4 wt.% Cr–3.1 wt.% Mn). Optical microscopy, scanning electron microscopy, energy-dispersive spectroscopy, X-ray diffraction analysis, microhardness measurements, and tribological tests were conducted for coating characterizations. It was found that after ten plasma pulses (under a discharge voltage of 4 kV) and post-plasma heat treatment (two hours of holding at 950 °C and oil-quenching), a coating (thickness = 210–250 µm) consisting of 48 vol.% Cr-rich carbides (M7C3, M3C), 48 vol.% martensite, and 4 vol.% retained austenite was formed. The microhardness of the coating ranged between 980 and 1180 HV. The above processes caused a gradient in alloying elements in the coating and the substrate due to the counter diffusion of C, Cr, and Mn atoms during post-plasma heat treatments and led to the formation of a transitional layer and different structural zones in near-surface layers of cast iron. As compared to gray cast iron (non-heat-treated and heat-treated), the coating had 3.0–3.2 times higher abrasive wear resistance and 1.2–1208.8 times higher dry-sliding wear resistance (depending on the counter-body material). The coating manifested a tendency of solidification cracking caused by tensile stress due to the formation of a mostly austenitic structure with a lower specific volume. Cracks facilitated abrasive wear and promoted surface spalling under dry-sliding against the diamond cone.