9 July 2022 in Materials Science and Engineering: A
4 March 2024 in Construction and Building Materials
1 January 2019 in Science and Technology of Welding and Joining
Dissimilar joint between 304L austenitic stainless steel and low-alloy steel 16Mn was underwater wet welded using self-shielded nickel-based tubular wire. Microstructure, mechanical properties and corrosion behaviour of dissimilar welded joints were discussed. Ni-based weld metal was fully austenitic with well-developed columnar sub-grains. Type II boundary existed between Ni-based weld metal and ferritic base metal in underwater welds similar to that in air welds. Major alloying elements distributed non-uniformly across the austenitic weld metal/16Mn interface. Maximum hardness values in wet welding appeared in a coarse-grained heat-affected zone at the 16Mn side, which possessed very low impact toughness. Underwater Ni-based welded joints fractured at Ni-based weld metal under tensile test. Ni-based weld metal had favourable corrosion resistance similar to 304L base metal.
14 May 2019 in Journal of the American Ceramic Society
1 September 2021 in Polish Maritime Research
The paper described the experimental findings of underwater wet welding of E40 steel using self-shielded flux-cored wire with a TiO 2 -FeO-MnO slag system. The arc stability, weld quality and corrosion resistance with different heat inputs were studied. The results showed that the wet welding process of the designed wire displayed good operability in the range of investigated parameters. The microstructure and mechanical properties of the weld metal depended on the heat input. Due to the high fraction of acicular ferrite in the weld metal, the mechanical properties of the weld metal under low heat input had better tensile strength and impact toughness. Fracture morphologies at low heat input had uniform and small dimples, which exhibited a ductile characteristic. The diffusible hydrogen content in the deposited metal obtained at a heat input of 26 kJ/cm significantly reduced to 14.6 ml/100g due to the combined effects of Fe 2 O 3 addition and the slow solidification rate of molten metal. The microstructure also had a significant effect on the corrosion resistance of the weld metal. The weld metal with high proportions of acicular ferrite at low heat input exhibited the lowest corrosion rate, while the base metal possessed a reduced corrosion resistance. These results were helpful to promote the application of low alloy high strength steel in the marine fields.
28 January 2026 in Advanced Composites and Hybrid Materials
Reliable brazing of C/C-SiC composites to stainless steel is hindered by severe residual stresses and uncontrolled interfacial reactions. Here, we introduce a CuMnCr/Mo/Cu multilayer interface that aims to simultaneously regulates stress distribution and interfacial chemistry. Cr from the CuMnCr layer preferentially reacts with C/C-SiC, forming a Cr7C3 + Cr3Si reaction layer, while Fe and Cr from stainless steel diffuse into Cu to produce a (Cu, Fe, Cr) solid solution. The Mo interlayer mainly acts as both a diffusion barrier and a compliant stress absorber, isolating reaction zones and concentrating part of the residual stress within itself. Finite-element simulations confirm that this design reduces peak Mises stress from 684 MPa to 444 MPa. At an optimized brazing temperature of 980 °C, the joint achieves a shear strength of 32.2 MPa, corresponding to 57.5% of the intrinsic strength of C/C-SiC. Thermodynamic, kinetic, and first-principles analyses suggest that Cr plays a dominant role in interfacial bonding, whereas Mo contributes to the redistribution of residual stress and mitigation of brittle fracture. Overall, this multilayer strategy provides mechanistic insight into how Cr-driven interfacial control can be combined with Mo-assisted stress management to design reliable C/C-SiC-metal joints, while the long-term service behavior and extension to other composite/steel combinations remain to be clarified in future work.