Yinan Xiao

Yinan Xiao

Auto-generated profile, based on publicly available information

Yinan Xiao

PKU-HKUST Shenzhen-HongKong Institution, Shenzhen 518057, China

Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 December 2022 in AIP Advances
Verified
Journal Article
Open access
PDF file
SCSiyuan Cheng
Siyuan Cheng
YXYinan Xiao
Yinan Xiao
XLXueshi Li
Xueshi Li
HLHongyang Lin
Hongyang Lin
PHPeng Hua
Peng Hua
QSQingping Sun
Qingping Sun
In this article, the elastocaloric effect of a commercial superelastic NiTi shape memory alloy (SMA) tube (with an outer diameter of 5 mm and wall thickness of 1 mm) to be applied in a compressive cooler was measured and analyzed. The elastocaloric effect of the tube was measured vs the applied strain and strain rate. The largest temperature changes of 21 K during loading and 16 K during unloading were measured at an applied strain of 3.30% and strain rate of 0.33 s−1. In the fatigue testing of the sample, only 0.20% of the residual strain accumulated after a runout of 1 × 106 sinusoidal force-controlled loading–unloading cycles at a maximum compressive stress of 1100 MPa and frequency of 20 Hz. Numerical results of the cooling characteristics of a compressive device using a single NiTi tube with the above-mentioned cross section and an aspect ratio of 60:1 as the refrigerant showed that the device could produce a total cooling power of up to 20 W and a coefficient of performance of up to 6.5. The results of this article demonstrate that superelastic NiTi SMA tubes of suitable wall thickness and aspect ratios are good candidates to be applied in a compressive elastocaloric cooler.

11 April 2024 in Archives of Metallurgy and Materials
Verified
Journal Article
Closed access
PDF file
QWQiaoli Wang
Qiaoli Wang
YXYinan Xiao
Yinan Xiao
DWDi Wu
Di Wu
FYFang Yang
Fang Yang
Liyuan ShengLiyuan Sheng
Liyuan Sheng
In the present research, the Nb-Si-Ti-Cr-Al-Ta-Hf alloys with different Ho addition were prepared. Their microstructure, compressive properties and oxidation behaviors were investigated preliminarily. The results exhibit that the Nb-Si-Ti-Cr-Al-Ta-Hf alloy has coarse microstructure which is mainly composed of Nb solid solution, Nb5Si3 and Ti5Si3 phases. The minor Ho addition could refine the microstructure and suppress the precipitation of Ti5Si3 phase. Moreover, the Ho addition also leads to the formation of Ho2Hf2O7, which prefers to precipitate along the Nbss/Nb5Si3 phase interface. Compared with the Nb-Si-Ti-Cr-Al-Ta-Hf alloy, the minor Ho addition improves the room-temperature and high-temperature compressive properties of the alloy. Its room-temperature compressive strength and ductility obtain the maximum value of 1825 MPa and 16.5% when the Ho content is 0.1 at.%. Moreover, its best compressive strength at 873 K, 1273 K and 1473 K is 1495 MPa, 765 MPa and 380 MPa, respectively, when the Ho addition is 0.1 at.%. The oxidation behavior of the Nb-Si-Ti-Cr-Al-Ta-Hf alloy is diversified with the Ho addition. The oxidation rate of the alloy with 0.1 at.% Ho addition is the lowest while the alloy with 0.2 at.% Ho addition is the highest. Therefore, the 0.1 at.% Ho would be the appropriate content for the Nb-Si-Ti-Cr-Al-Ta-Hf alloy.