Franjo Kozina

Franjo Kozina

Auto-generated profile, based on publicly available information

Franjo Kozina

University of Zagreb, Faculty of Metallurgy, Sisak, Croatia

Research Focus & Metrics

Academic Career Length

9Years (2018-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
10 October 2018 in Archives of Metallurgy and Materials
Verified
Journal Article
Open access
PDF file
ZGZ. Glavas
Z. Glavas
ASA. Strkalj
A. Strkalj
KMK. Maldini
K. Maldini
FKF. Kozina
F. Kozina
Effects of additions of 0.00064, 0.001 and 0.0042 wt.% Bi on the graphite structure in the section thicknesses of 3, 12, 25, 38, 50, 75 and 100 mm of spheroidal graphite cast iron castings containing 2.11 wt.% Si and rare earth (RE) elements (Ce + La + Nd + Pr + Sm + Gd) in the range from 0.00297 to 0.00337 wt.% were analyzed in this paper. Addition of Bi was not necessary for obtaining high nodule count and nodularity higher than 80% in section thicknesses of 3, 12 and 25 mm. RE elements showed a beneficial effect on the nodule count and nodularity in these sections. Nodularity was below 80% in section thicknesses of 38, 50, 75 and 100 mm when Bi was not added. Detrimental effect of RE elements on graphite morphology in these sections was neutralized by adequate addition of Bi. Addition of 0.001 wt.% Bi (ratio of RE/Bi = 3.27) was enough to achieve nodularity above 80% in the section thickness of 38 mm. Nodularity was increased above 80% in section thicknesses of 50, 75 and 100 mm by addition of 0.0042 wt.% Bi (ratio of RE/Bi = 0.78). At the same time, Bi significantly increased the nodule count. Nodularity above 80% and the high nodule count in the section thicknesses of 75 and 100 mm were also achieved by using an external metallic chill in the mold. In this case, addition of Bi was not required.

1 January 2020 in Journal of Mining and Metallurgy, Section B: Metallurgy
Verified
Journal Article
Open access
PDF file
FKF. Kozina
F. Kozina
Zdenka Zovko BrodaracZdenka Zovko Brodarac
Zdenka Zovko Brodarac
Mitja PetričMitja Petrič
Mitja Petrič
APA. Penko
A. Penko
As a major impurity element in aluminium-lithium (Al-Li) alloys, iron (Fe) reduces formability, fracture toughness, and fatigue resistance by solidifying into Al6Fe and Al3Fe particles. The research was performed in order to estimate the influence of Fe impurities on the compression behaviour of Al-2.24Mg-2.09Li alloy. The investigation was performed on the samples in as cast and solution hardened condition. The solution hardening was applied to improve the mechanical properties by dissolving intermetallic particles and enriching ?Al matrix with Mg. However, the higher strength properties and temperature increase during the compression testing were observed in as cast condition. Microstructural investigation revealed significant differences in microstructure changes between the samples in as cast and solution hardened condition. In as cast sample the barrelling effect led to the unequal deformation and surface texture development. The eutectic Al3Fe particles located in the ?Al interdendritic areas did not significantly impact microstructure changes. Although the solution hardening led to enrichment of ?Al matrix with Mg and Fe, the Al3Fe particles were not dissolved. The coarse morphology of Al3Fe particles and location at the grain boundaries of ?Al grains contributed to low energy intergranular fracture. The fracture nucleation and propagation across the grain boundaries resulted in lower strength values.

26 May 2025 in Metallurgical & Materials Engineering Congress of South-East Europe
Verified
Journal Article
Closed access
NDNatalija Dolić
Natalija Dolić
Zdenka Zovko BrodaracZdenka Zovko Brodarac
Zdenka Zovko Brodarac
FKFranjo Kozina
Franjo Kozina
In this work, the hardness homogeneity of aluminum Al-Mg alloy slabs produced with semicontinuous casting process from 6 different charges was investigated. The evaluation of hardness homogeneity was carried out on the front and rear cross-sectional plates of the slabs at locations determined by a statistical design of experiments (“Latin square”). Previous studies have shown that the hardness depends on the location of the test and also correlates with the technological conditions. Therefore, hardness measurements were carried out according to the Vickers method at different distances from the edge of the plate: 1 mm, 2 mm, 5 mm, 10 mm and 20 mm. The hardness of the tested aluminum alloy plates decreases in both the height and width of the plate from the edges to the center, following the polynomial behavior. The hardness decreases from the edge up to a distance of 5 mm, after which the hardness equalizes for both for the slabs’ fronts and rears.

1 January 2026 in Journal of Mining and Metallurgy, Section B: Metallurgy
Verified
Journal Article
Open access
NDNatalija Dolić
Natalija Dolić
Zdenka Zovko BrodaracZdenka Zovko Brodarac
Zdenka Zovko Brodarac
FKFranjo Kozina
Franjo Kozina
This study examines the spatial variability of HV5 hardness in industrially produced Direct Chill (DC) cast EN AW-5083 aluminium alloy ingots in the as-cast and homogenized conditions. Hardness measurements were performed at predefined sampling positions in the front and rear sections of six ingots using a Latin square design and evaluated by analysis of variance (ANOVA), coefficients of variation, correlation analysis, and linear regression. The results indicate a uniform longitudinal hardness distribution, with similar mean HV5 values at the front and rear sections, while significantly larger variations occur across the ingot cross-section. Slice height (i) and slice width (j) were identified as the dominant sources of variability. Homogenization reduced the overall mean HV5 from 81.8 HV5 to 75.7 HV5, decreased the coefficient of variation from 5.56% to 4.64%, and increased the correlation coefficient from r = 0.76 to r = 0.85. A statistically significant but limited relationship between the number of grains per unit area (NA) and hardness was observed, indicating that NA contributes to local hardness variations but is not the dominant factor controlling the overall spatial hardness distribution. The results indicate that homogenization does not increase hardness but improves its spatial homogeneity primarily through reduction of local microstructural and compositional heterogeneity.

1 January 2026
Verified
Conference Paper
Open access
PDF file
NDNatalija Dolić
Natalija Dolić
Zdenka Zovko BrodaracZdenka Zovko Brodarac
Zdenka Zovko Brodarac
LMLucija Majdandžić
Lucija Majdandžić
LMLuka Mesek
Luka Mesek
FKFranjo Kozina
Franjo Kozina
EN 1.2709 (EOS MaragingSteel MS1) was processed by Selective Laser Melting in the x-y orientation, with gauge sections built from 325 and 250 layers. The as-built microstructure consists of lath martensite in packets delineated by melt-pool boundaries and is identical for both layer numbers. Fracture is ductile, by micro-void coalescence, and the fibrous area fraction increases with the number of layers. The material reaches Rm = 1197-1201 MPa, Rp0.2 = 1059-1072 MPa, A = 16.5-18.0 % and Z = 61-66,5 %. The strength lies within the scatter band specified for the as-built condition and the elongation at or above its upper bound.

1 January 2025
Verified
Conference Paper
Open access
PDF file
FKFranjo Kozina
Franjo Kozina
Zdenka Zovko BrodaracZdenka Zovko Brodarac
Zdenka Zovko Brodarac
IBIvica Buljeta
Ivica Buljeta
NDNatalija Dolić
Natalija Dolić
When manufacturing components with high safety-critical requirements, integrity and reliability must be guaranteed despite the possibility of systemic or random failures. This is complicated by the fact that any of these failures may be caused by random defects inherent in the manufacturing process or operating conditions. The investigation was performed to determine the cause of a permanent random failure in the form of a crack observed during the manufacture and testing of an AlSi11 automotive rim. By correlating the results of chemical composition analysis, thermodynamic calculations, and metallographic analysis, it was found that the crack nucleated on the previously formed shrinkage porosity and propagated across the non-metallic inclusions, the over-modified eutectic (a Al + b Si), Al 5FeSi (b) and Al 8FeMg 3Si 6 (p) phases with characteristic morphologies.