Two-dimensional (2D) ferroelectrics refer to those ferroelectrics with layered structure and weak interlayer interactions (e.g., van de Waals interlayer coupling). A number of basic physical issues in the framework of ferroelectricity deserve clarifications, and one of them is the size effect regarding the dependence of ferroelectricity on material thickness. In this work, we investigate the ferroelectric domain structures of 2D ferroelectric CuInP2S6 nanoflakes attached on heavily doped Si wafers and polarization switching using the piezoresponse force microscopy. While the domain structure shows highly irregular morphology and 180° domain walls, the statistics on domain size (diameter) W and nanoflake thickness d demonstrates the remarkable thickness dependence of domain size, illustrated by the shrinking domain size from 630 nm to 75 nm with decreasing thickness d from ∼130 nm to ∼11 nm. This dependence fits the Landau-Lifshitz-Kittel (LLK) scaling law with the scaling exponent of ∼0.65, slightly larger than 0.5 for 3D ferroelectrics. It is suggested that the size effect in terms of the LLK scaling law does not show an essential difference between the 2D and 3D ferroelectric systems.
The increasing miniaturization of electronics requires a better understanding of material properties at the nanoscale. Many studies have shown that there is a ferroelectric size limit in oxides, below which the ferroelectricity will be strongly suppressed due to the depolarization field, and whether such a limit still exists in the absence of the depolarization field remains unclear. Here, by applying uniaxial strain, we obtain pure in-plane polarized ferroelectricity in ultrathin membranes, providing a clean system with high tunability to explore ferroelectric size effects especially the thickness-dependent ferroelectric instability with no depolarization field. Surprisingly, the domain size, ferroelectric transition temperature, and critical strain for room-temperature ferroelectricity all exhibit significant thickness dependence. These results indicate that the stability of ferroelectricity is suppressed (enhanced) by increasing the surface or bulk ratio (strain), which can be explained by considering the thickness-dependent dipole-dipole interactions within the transverse Ising model. Our study provides new insights into ferroelectric size effects and sheds light on the applications of ferroelectric thin films in nanoelectronics.
1 June 2021 in Journal of the Taiwan Institute of Chemical Engineers
When the stoichiometric proportion of Cu in Ca4 − xCuxTi4O12 polycrystalline ceramics is decreased from 3 to 2 and then to 1, the room-temperature permittivity is reduced by one order of magnitude during each step. Ca/Cu atomic disorder is observed only in some grains of Ca3CuTi4O12 single-phase polycrystalline ceramics, and the disorder is not the origin of the giant permittivity in CaCu3Ti4O12. Quantitatively, the permittivity magnitude is related to the mole ratio of polaronlike 3d electrons from Cu ions.
In the CaCu3TiO4 solid bulks with the giant permittivity of ∼104, the 100-fold permittivity-drop below 200 K has been observed without any long-range structural transition. In the frame of the comprehensive model, the Ising-model analysis of dielectric polarization is applied and the energy of the nearest interaction among the dipoles is deduced from the experiments by utilizing the particle swarm optimization. The interaction energy of ∼56 meV is reasonably smaller than the experimental value of the thermal activation energy of ∼88 meV. The interaction energy is independent of the temperatures, the dipole-chain lengths, and the frequencies of the applied AC electric field. Therefore, such appropriate, stable, and intrinsic interaction energy makes the many-body dielectric relaxation rather than the structural transition responsible for the permittivity drop.
In-plane electrical impedance has been examined in as-grown single crystals of BaFe2As2, one of the parent compounds of iron-based superconductors. From the results, it is found that the real part of the impeditivity, namely the AC resistivity, reveals the in-plane anisotropy of the material without any applied uniaxial strain. The imaginary part, i.e., the reactivity, also indicates strong in-plane anisotropy and is linearly dependent on the electrical frequency. Our study demonstrates that electrical impedance is a new and effective method of probing the electron nematicity of iron-based superconductors.