6 July 2010 in Nanotechnology
We demonstrate the fabrication of N-face GaN nanorods by metal organic vapour phase epitaxy (MOVPE), using continuous-flux conditions. This is in contrast to other approaches reported so far, which have been based on growth modes far off the conventional growth regimes. For position control of nanorods an SiO(2) masking layer with a dense hole pattern on a c-plane sapphire substrate was used. Nanorods with InGaN/GaN heterostructures have been grown catalyst-free. High growth rates up to 25 microm h(-1) were observed and a well-adjusted carrier gas mixture between hydrogen and nitrogen enabled homogeneous nanorod diameters down to 220 nm with aspect ratios of approximately 8:1. The structural quality and defect progression within nanorods were determined by transmission electron microscopy (TEM). Different emission energies for InGaN quantum wells (QWs) could be assigned to different side facets by room temperature cathodoluminescence (CL) measurements.
1 October 2014 in Journal of Physics D: Applied Physics
30 January 2012 in Physical Review B
GaAs nanowires (NWs) grown by molecular-beam epitaxy may contain segments of both the zincblende (ZB) and wurtzite (WZ) phases. Depending on the growth conditions, we find that optical emission of such NWs occurs either predominantly above or below the band gap energy of ZB GaAs (EgZB). This result is consistent with the assumption that the band gap energy of wurtzite GaAs (EgWZ) is larger than EgZB and that GaAs NWs with alternating ZB and WZ segments along the wire axis establish a type II band alignment, where electrons captured within the ZB segments recombine with holes of the neighboring WZ segments. Thus, the corresponding transition energy depends on the degree of confinement of the electrons, and transition energies exceeding EgZB are possible for very thin ZB segments. At low temperatures, the incorporation of carbon acceptors plays a major role in determining the spectral profile as these can effectively bind holes in the ZB segments. From cathodoluminescence measurements of single GaAs NWs performed at room temperature, we deduce a lower bound of 55 meV for the difference EgWZ$-${}EgZB.
9 August 2012 in Physical Review B
We present a universal approach for determining the spontaneous polarization Psp of a wurtzite semiconductor from the emission energies of excitons bound to the different types of stacking faults in these crystals. Employing microphotoluminescence and cathodoluminescence spectroscopy, we observe emission lines from the intrinsic and extrinsic stacking faults in strain-free GaN microcrystals. By treating the polarization sheet charges associated with these stacking faults as a plate capacitor, Psp can be obtained from the observed transition energies with no additional assumptions. Self-consistent Poisson-Schr\"odinger calculations, aided by the microscopic electrostatic potential computed using density-functional theory, lead to nearly identical values for Psp. Our recommended value for Psp of GaN is $-${}0.022\ifmmode\pm\else\textpm\fi{}0.007 C/m2.
7 November 2017 in Physical Review Letters
We observe that the growth rate of in plasma-assisted molecular beam epitaxy can be drastically enhanced by an additional In supply. This enhancement is shown to result from a catalytic effect, namely, the rapid formation of , immediately followed by a transformation of to due to an In-Ga interatomic exchange. We derive a simple model that quantitatively describes this process as well as its consequences on the formation rate of . Moreover, we demonstrate that the catalytic action of allows the synthesis of the metastable hexagonal phase of . Since the interface is closely lattice matched, this novel growth mode opens a new path for the fabrication of sesquioxide heterostructures.
5 August 2011 in Crystal Growth & Design