Different concentrations of powdered aluminum (Al) or cerium sulfate in the range between 10 and 60 phr were incorporated into styrene-butadiene rubber (SBR) matrices. The physico-mechanical and electrical properties of vulcanizates were measured and evaluated. An improvement in the mechanical properties according to increased filler loading in SBR composites was noted. This finding is reinforced by filler dispersion values (Lee equation), reinforcing index and thermal analysis. The dielectric properties, namely the relative permittivity (ε') and dielectric loss (ε”), were measured as function of both frequency and concentration of the SBR/filler composites. The results showed an enhancement in the dielectric and mechanical properties, especially for Al powder. This is due to the enhancement of filler-rubber interactions and the continuity of the conductive phase through the composites. The SEM micrograph showed that the filler agglomerates were dispersed within the SBR matrix.
28 August 2015 in Journal of Materials Science and Engineering B
The current research presentsthe development of EPDM rubber including shape memory alloy. The Cu-Al-Zn alloy was modified with the coupling agent3-(Trimethoxysilyl) propyl methacrylate (TMSPM)and then incorporated into Ethylene propylene diene rubber (EPDM) by a 2-roll mill technique.The Cu-alloy behaved as superelasticity capability which can be used in various engineering approaches to smart materials. Microstructure, mechanical, rheological and magnetic properties of Cu-Al-Zn/EPDM composites was studied. The rheometericresults indicated that the incorporation of Cu-Al-Zn as a fillerenhance the curing process. Howeverthecuring time ofCu-Al-Zn/EPDMcomposites was reduced compared to the control sample without Cu-alloy. For the mechanical properties, increasing Cu-alloy loading inthe EPDMcomposites resulted inan increment of elongation at break.The addition of Cu based alloy as fillers improved the magnetization of composites with coupling agent when compared toEPDM rubber and Cu-Al-Zn/EPDMcomposites without coupling agent.
18 November 2014 in The European Physical Journal Applied Physics
The effects of 1, 3 and 5 wt.% Cu additions on structure, Vickers hardness, indentation creep and corrosion behaviour of Al-5Ti-1B ternary alloy were studied and analyzed. The Al-5Ti-1B alloy exhibited a mixture of Al3Ti and TiB2 intermetallic compounds (IMCs), and Al solid solution. Additions of 1 and 3 wt.% Cu showed the same phases, indicating a complete solubility of Cu atoms in Al matrix. In addition, the Al-5Ti-1B-5Cu alloy exhibited a precipitation of CuAl2 IMC. Furthermore, additions of Cu decreased the particle size of Al matrix. This structural behaviour increased rapidly the Vickers hardness number (HV) from 643 to 1395 MPa, increased the indentation creep resistance and improved corrosion behaviour of the Al-5Ti-1B alloy. Cu is anti-corrosion phase when completely dissolved or precipitated as IMC in Al matrix.
Molecular modeling is utilized at D-Gauss level to calculate vibrational frequencies, band gap energy and thermal parameters for Al–Sn–Cu alloy. Some physical parameters of the studied structure are calculated at PM3 semiemperical quantum mechanical method. Based on modeling work, experimental work is conducted upon for Al–Sn–Cu alloy to study the effect of cold rolling and heat treatment on the microstructure and microhardness (Hv). Results indicate the following; Hv was increased with annealing temperature up to 230 °C and then decreased with further increasing temperature. This behavior takes place because of the solid solution strengthening of the α-Al matrix followed by reduce of precipitation hardening and vanishing of vacancies. This was discussed by the role of microstructure to explain thermal properties and its relation to microhardness.