14 November 2019 in Scientific Reports
Phosphor-converted white light-emitting diodes (pc-WLEDs) are excellent energy-efficient light sources for artificial lighting applications. One goal of artificial lighting is to make objects/images look natural – as they look under the sunlight. The ability of a light source to accurately render the natural color of an object is gauged by the parameter – color rendering index (CRI). A conventional pc-WLED has an average CRI ~ 80, which is very low for accurate color reproduction. To utilize the pc-WLEDs for artificial lighting applications, all the CRI points (R1 – R15) should be above 95. However, there is a trade-off between CRI and luminous efficacy (LER), and it is challenging to increase both CRI and LER. Herein we propose a novel LED package (PKG) design to achieve CRI points ≥95 and efficiency ~100 lm/W by introducing two blue LEDs and a UV LED in combination with green and red phosphors. The silicone encapsulant, the current through the LEDs, and the green/red phosphor ratio were optimized for achieving high CRI and LER. Our re-designed LED PKG will find applications in stadium lighting as well as for ultra-high-definition television production where high CRI points are required for the artificial light source.
10 February 2016 in Optical Materials Express
Optical properties of the line-emitting K2SiF6:Mn4+ phosphor were investigated for LED application. The color coordinate on the CIE chromaticity diagram, photoluminescence (PL), excitation characteristics and decay time of the K2SiF6:Mn4+ phosphor were measured and compared with those of the CaAlSiN3:Eu2+ red phosphor. Then, a set of white LEDs were fabricated based on these two red phosphors. The K2SiF6:Mn4+-loaded white LED is found to have big advantages over the CaAlSiN3:Eu2+-loaded white LED in the luminous flux and the color gamut. Its longevity and the color variation are inferior to its counterpart at 85°C, 85% relative humidity test. However, it is demonstrated in this work that they are improved much by blending two phosphors for white LED application while keeping its performance. Also, it is discussed on how longevity of the K2SiF6:Mn4+ phosphor is improved.
24 August 2012 in Optical Materials Express
Optics InfoBase is the Optical Society's online library for flagship journals, partnered and copublished journals, and recent proceedings from OSA conferences.
27 September 2016 in Scientific Reports
The long-term instability of the presently available best commercial phosphor-converted light-emitting diodes (pcLEDs) is the most serious obstacle for the realization of low-cost and energy-saving lighting applications. Emission from pcLEDs starts to degrade after approximately 200 h of operation because of thermal degradation of the phosphors. We propose a new strategy to overcome this thermal degradation problem of phosphors by wrapping the phosphor particles with reduced graphene oxide (rGO). Through the rGO wrapping, we have succeeded in controlling the thermal degradation of phosphors and improving the stability of fabricated pcLEDs. We have fabricated pcLEDs with long-term stability that maintain nearly 98% of their initial luminescence emission intensity even after 800 h of continuous operation at 85 °C and 85% relative humidity. The pcLEDs fabricated using SrBaSi2O2N2:Eu2+ phosphor particles wrapped with reduced graphene oxide are thermally stable because of enhanced heat dissipation that prevents the ionization of Eu2+ to Eu3+. We believe that this technique can be applied to other rare-earth doped phosphors for the realization of highly efficient and stable white LEDs.
2 July 2016 in Journal of Information Display
1 January 2008 in Journal of the Electrochemical Society
To improve the longevity of a phosphor converted white light-emitting diode (LED), the coating on CaS:Eu phosphor by using polymer binder was carried out. The coating characteristics were found to be critically dependent on the sort of monomer and temperature of the reaction during the polymerizing process. This process is found to avoid a hydrolysis reaction, which causes damage to CaS:Eu phosphor surface, which frequently occurs in the conventional sol-gel process. Field-emission scanning electron microscope images and transmission electron microscopy images showed that polymer binder coating of on CaS:Eu phosphor was very solid and could well serve as a protective layer against the moisture, which is critically detrimental to the development of commercial white LEDs. Significant optical stability, even after a moisture-contacting experiment, was observed in the case of coated phosphors. However, it was also found that the emission of from the CaS:Eu phosphor still remained influential to the longevity of an LED device because of a bottom Ag plate in our experimental regime.