Hydrogen embrittlement (HE) susceptibility was evaluated on JIS–SUP12-based steel (SB), and V-, Nb- and (Nb+Mo)-added steels (SV, SNb and SNbMo, respectively) under uniaxial tension and high stress triaxiality conditions, to elucidate the roles of the microalloying elements in the HE mechanisms of 2 GPa-grade medium-carbon Si–Cr spring steels, which were obtained via low-temperature tempering. The SV steel contained solute V and undissolved V carbides, the SNb steel undissolved Nb carbides and the SNbMo steel solute Mo and undissolved Nb carbides. The microalloying of V, Nb and Mo decreased the apparent hydrogen diffusivity owing to strong hydrogen attraction by solute V and Mo, and reversible hydrogen trapping with V and Nb carbides. Although all the steels attained the 2 GPa tensile strength in hydrogen-uncharged state, hydrogen significantly reduced the tensile strength through premature failure before the onset of yielding under uniaxial tension condition. In the hydrogen-charged specimens, the strength was strongly correlated with the shear fracture surface area. The HE susceptibility was increased in the following order: SNbMo ≈ SNb < SB < SV. This suggests that hydrogen-induced plasticity mitigates the HE susceptibility in the SNb and SNbMo steels, whereas the solute V facilitates the hydrogen-induced plastic inhomogeneity, which leads to premature fracture. Under high stress triaxiality condition in micro-cantilever specimens, hydrogen decreased the intrinsic fracture resistance to one third compared to the uncharged specimens, regardless of the steels. In the microalloyed specimens, hydrogen suppressed intergranular fracture, whereas the dependence of fracture resistance on the microalloying element was minor.
Hydrogen embrittlement (HE) susceptibility was evaluated on JIS-SUP12-based steel (SB), and V-, Nb- and (Nb+Mo)-added steels (SV, SNb and SNbMo, respectively) under uniaxial tension and high stress triaxiality conditions, to elucidate the roles of the microalloying elements in the HE mechanisms of 2 GPa-grade medium-carbon Si–Cr spring steels, which were obtained via low-temperature tempering. The SV steel contained solute V and undissolved V carbides, the SNb steel undissolved Nb carbides and the SNbMo steel solute Mo and undissolved Nb carbides. The microalloying of V, Nb and Mo decreased the apparent hydrogen diffusivity owing to strong hydrogen attraction by solute V and Mo, and reversible hydrogen trapping with V and Nb carbides. Although all the steels attained the 2 GPa tensile strength in an uncharged state, hydrogen significantly reduced the tensile strength through premature failure before the onset of yielding under uniaxial tension condition. In the hydrogen-charged specimens, the strength was strongly correlated with the shear fracture surface area. The HE susceptibility was increased in the following order: SNbMo ≈ SNb < SB < SV. This suggests that hydrogen-induced plasticity mitigates the HE susceptibility in the SNb and SNbMo steels, whereas the solute V facilitates the hydrogen-induced plastic inhomogeneity, which leads to premature fracture. Under high stress triaxiality condition in micro-cantilever specimens, hydrogen decreased the intrinsic fracture resistance to one third compared to the uncharged specimens, regardless of the steels. In the microalloyed specimens, hydrogen suppressed intergranular fracture, whereas the dependence of fracture resistance on the microalloying element was minor.
Microtensile tests combined with crystal plasticity finite element simulations were performed on a single-packet structure of a nano-bainite steel. The steel microstructure consisted of bainitic ferrite and retained austenite, and its constituents were formed according to the Nishiyama–Wassermann crystallographic orientation relationship. The single-packet specimens exhibited plastic anisotropy in their yielding behavior, similar to those of lath martensite and upper bainite. The deformation-induced transformed martensite variants demonstrated high kernel average misorientation values owing to the introduction of a large number of dislocations, and these crystallographic orientations were similar to those of the adjacent bainite variants, in which the slip system with the highest Schmid factor was nearly parallel to the transformation system. A numerical analysis incorporating a crystal plasticity constitutive model that accounted for the martensitic transformation closely represented experimental stress–strain responses, demonstrating the effectiveness of the proposed method. When applied to polycrystalline structures, multiaxial stress distributions promoted martensitic transformations, leading to significant strain hardening. Assuming a high austenite strength in the analysis model, the strength increased owing to the bainitic matrix, whereas strain hardening was limited because of the suppressed martensitic transformation. In contrast, assuming low-strength austenite in the model, the yield stress was slightly reduced while the martensitic transformation was enhanced, which resulted in pronounced strain hardening and a high tensile strength. These findings suggest that the incorporation of low-strength austenite within a high-strength matrix can optimize the balance between strength and ductility.