Zinc zirconate nanocomposite was synthesized by a low-temperature solution combustion method using citric acid as fuel at a pH of 7. The synthesis was done by varying the ratios of zirconium butoxide and zinc nitrate, which were the precursors in this study. The samples were calcined at 600 °C for 2 h then their structural and optical characteristics investigated. The analysis showed that the nanocomposite consisted of mixed phases of zinc zirconate, zinc oxide, and zirconium oxide. As the Zn2+/Zr4+ ratio increased, the highly agglomerated morphologies gradually developed crystalline aggregates mixed with nanorods. A red-shifted blue emission with a peak at 409 nm was observed in the photoluminescence spectra and the composites had an energy bandgap between 2.81 and 3.12 eV.
Zinc zirconate nanocomposites with varying compositions of Dy3+ ions were synthesized through a solution combustion method using citric acid as a fuel. There were mixed hexagonal ZnO and cubic ZrO2 phases in the X-ray diffraction patterns of the composites whose average crystallite sizes range between 27 and 38 nm. Scanning electron microscopy images show a mixture of polygonal and hexagonal rod-like structures of varying aggregation levels at the different Dy3+ -doping concentrations. The reflectance spectra showed absorption edges around 400 nm and an energy bandgap between 2.99 and 3.07 eV. There was a violet emission from the host matrix that gradually shifted towards white light with enhanced doping. At a higher Dy3+ concentration, there was luminescence quenching attributed to dipole-dipole interaction among the dopant ions. The synthesized nanocomposite phosphors may be used in sensors and colored display technology.
The nanocomposites were prepared using varying concentrations of ions through the solution combustion method. Zirconium butoxide and zinc nitrate were used as the precursor solutions with citric acid as a fuel. The synthesis was done at a low temperature of 80°C and then the samples calcined at 600°C for 2 h, before characterization. Rietveld refinement revealed that the nanocomposite consisted of wurtzite zinc oxide, mixed with cubic and tetragonal zirconia phases. Scanning electron microscopy images show dispersed small polygonal crystals within a spongy matrix for lower concentrations, while samples with higher dopant ratios featured larger crystals mixed with rods. The UV spectra had absorption edges from 400 nm with a dopant-dependent energy band gap ranging between 2.78 and 3.04 eV. The nanocomposites exhibited an initial violet emission that varied through blue into the green region, depending on the doping concentration. Dipole–dipole interaction was found to be responsible for the luminescence quenching within the nanocomposite material.