The objective was to evaluate the color stability of ceramic veneers luted with resin cements and pre-heated composite resins (60oC) for 12 months, and determine the degree of conversion (DC) of the luting agents. Two resin cements (AllCem Veneer, light-cured (LRC) and AllCem, dual-cured (DRC)] and three composite resins [Z100 (MNCR-minifilled), Herculite Classic (MHCR-micro-hybrid) and Durafill (MCCR-microfilled)] were used for cementing 0.8-mm-thick lithium-silicate glass-ceramic laminates (Suprinity, shade B2-HT, Vita) on bovine enamel (n=10). The specimens were stored at 37oC in distilled water. CIELab parameters were determined at 24h after luting (baseline), 7, 30, 90, 180 days and 12 months. Three specimens were prepared for DC evaluation, performed by micro-Raman spectroscopy. Data were analyzed by ANOVA and Tukey’s test (a=5%). For ΔEab and ΔE00, there were significant differences for luting material (p<0.001), time (p<0.001), and double interaction (p<0.001). The groups cemented with MHCR (1 year), MCCR (90 days and 1 year) and MCCR-PH (1 year) were the ones with ΔE values greater than the acceptability threshold. All other groups maintained their ΔE lower than the acceptability threshold after 1 year in distilled water. Regarding DC, there were no significant differences (p=0.127) among the materials. Non-significant negative correlations were observed between the mean ΔEab and DC (R=-0.65) and ΔE00 and DC (R=-0.64). A significant positive correlation was observed mean ΔEab and ΔE00 (R=0.99). It was concluded that the different luting agents influenced the final color of the restorations. The heating of the composite resins did not affect their DC.
14 January 2017 in The Journal of Prosthetic Dentistry
The aim of this study was to evaluate the discoloration effects of water, cola-based soft drink, coffee, and wine on resin composites used in restorative dentistry and the possibility of removing the stain with chair side manual polishing. The A2 shade of three materials was tested. Disc specimens were prepared. A spectrophotometer was used to measure the baseline CIE-Lab color parameters of each material () 24 hours after sample preparation. Samples were then immersed in a cola-based soft drink, coffee, or wine for 1 hour every day, for 30 days. For the remaining hours, the specimens were stored in distilled water. In the control group, the specimens were immersed in water for the whole period. The color differences () were calculated after 7 and 30 days of storage, and after polishing with coarse Sof-Lex discs, and analyzed by two-way ANOVA with repeated measures and Tukey’s HSD test (). Luna presented higher values followed by Durafill and Herculite . For the drink solutions, values were higher for wine followed by coffee and for cola-based soft drink and water which were statistically similar. For time, values were higher for 30 days and then for 7 days and after polishing . The results indicate that color stability is material dependent. The types of drinks that patients consume also influence the color stability of restorative materials.