1 October 2017 in Materials Science and Technology
The effects of Cu and Al addition on the microstructure and fracture in the coarse-grained heat-affected zone (CGHAZ) of high-strength low-alloy steels with superior toughness were studied and compared with the X70 pipeline base steel counterpart. The microstructure in base steel was dominated by a small fraction of acicular ferrite and predominantly bainite. However, acicular ferrite microstructure was obtained in Cu-bearing steel, which nucleated on complex oxide with outer layer of MnS and CuS because of Cu addition. The microstructure in Al-bearing steel consisted of bainite with ultrafine martensite–austenite constituent, which was refined by Al addition. CGHAZ in Cu-bearing and Al-bearing steels had superior impact toughness and ductile fracture, which were attributed to acicular ferrite and ultrafine martensite–austenite constituent, respectively.
7 February 2023 in Construction and Building Materials
4 March 2019 in Heat Treatment and Surface Engineering
A Fe–0.20C–1.49Mn1.52Si–0.58Cr–0.05Nb low-carbon steel was treated by a novel quenching-partitioning-tempering (Q-P-T) process and the traditional quenching and tempering (Q&T) process for comparison, respectively. X-ray diffraction results indicate that there is 10.8% volume fraction of retained austenite (VRA) in the Q-P-T martensitic steel, while no diffraction peak of retained austenite was detected in Q&T martensitic steel. The Q-P-T steel and the Q&T steel were subjected to a dynamic tensile test at a strain rate of 500 s−1 and a quasi-static tensile test at a strain rate of 5.6 × 10−4 s−1, respectively. The results indicate that the high strain rate in the dynamic tension raises the strength of the Q-P-T and Q&T steels compared with their quasi-static tensions owing to strain rate hardening effect, however, the elongation of Q-P-T steel decreases slightly, while the elongation of Q&T steel evidently increases. This difference is attributed that the existence of the dislocation absorption by the retained austenite (DARA) effect in quasi-static tension is suppressed under dynamic tensile loading so that the enhancement influence of DARA effect on ductility cannot be effectively compensated by the adiabatic softening of the martensitic matrix, which leads to a slight decrease in the elongation of the Q-P-T steel in dynamic tension compared with that in the quasi-static tension. While Q&T steel has no DARA effect in quasi-static tension due to no retained austenite, and thus the adiabatic softening of the martensitic matrix increases the ductility of Q&T steel in dynamic tension.