1 March 2015 in Progress in Materials Science
15 May 2012 in Journal of Applied Physics
REBa2Cu3Oy (RE123 or REBCO, RE = rare earth elements) bulk high-temperature superconductors have a potential perspective for large-scale engineering applications. However, the cost of REBCO bulk production is rather high, considering high failure rates, expensive RE materials, and Pt or Ag addition. Using the cold-seeding in the top-seeded melt growth, a simple and feasible process, we succeeded in recycling the failed REBCO (RE = Y) bulks. The distinctive feature of this recycling process is the use of YBCO-buffered NdBCO films as seeds, which have high thermal stability and can endure a maximum processing temperature (Tmax) up to 1120 °C to enable full decomposition of solid REBCO. Three typical microstructures were recognized in the failed samples attributed to the inherent differences in the non-optimized growth heating profiles. Preferential recycling procedures were chosen according to the difficulty of the failed-samples decomposition, which has a certain connection with the microstructures of the failed bulks. Finally, after oxygenation, the recycled bulks demonstrate good superconducting properties.
28 October 2010 in Superconductor Science and Technology
25 April 2005 in Superconductor Science and Technology
2 June 2009 in Superconductor Science and Technology
15 July 2010 in Journal of Applied Physics
Y–Ba–Cu–O (YBCO) and Sm–Ba–Cu–O thin films have been used for the first time as heterogeneous seeds to multiseed successfully the melt growth of bulk YBCO in a multiseeded melt growth process. The use of thin film seeds, which may be prepared with highly controlled orientation (i.e., with a well-defined a-b plane and precisely known a-direction), is based on their superheating properties and reduces significantly contamination of the bulk sample by the seed material. A variety of grain boundaries were obtained by varying the angle between the seeds. Microstructural studies indicate that the extent of residual melt deposited at the grain boundary decreases with increasing grain boundary contact angle. It is established that the growth front proceeds continuously at the (110)/(110) grain boundary without trapping liquid, which leads to the formation of a clean grain boundary.