Aleksandr S. Andreenko

Aleksandr S. Andreenko

Auto-generated profile, based on publicly available information

Aleksandr S. Andreenko

LLC “MEM”, 123458 Moscow, Russia

Research Focus & Metrics

Academic Career Length

10Years (2017-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
28 November 2020 in Materials
Verified
Journal Article
Open access
PDF file
ADAndrey Dormidontov
Andrey Dormidontov
NKNatalia Kolchugina
Natalia Kolchugina
NDNikolay A. Dormidontov
Nikolay A. Dormidontov
YMYury V. Milov
Yury V. Milov
AAAlexander S. Andreenko
Alexander S. Andreenko
Experimental series of alloys for (Sm,Zr)(Co,Cu,Fe)Z permanent magnets are presented in the concentration ranges that provide wide variations of (4f)/(4d)/(3d) ratios of comprising elements. Optical metallographic analysis, observation of the surface domain structure upon magnetization reversal (Kerr effect), electron microprobe analysis, and measuring the major hysteresis loops of samples at different stages of heat treatment are used to study processes related to the development of the highly coercive state of these samples. It was found that the volume fractions of two main structural components A and B, which comprise 90% of the total sample volume, rigorously control the coercivity at all stages of thermal aging. At the same time, structural components A and B themselves in samples being in the high-coercivity state differ qualitatively and quantitatively in the chemical composition, domain structure and its development in external magnetic fields and, therefore, are characterized by different morphologies of the phases comprising the structural components. Two stages of phase transformations in the sample structure are observed. During isothermal annealing, the cellular structure develops within the B component, whereas, during stepwise (slow) cooling or quenching from the isothermal aging temperature to 400 °C, a phase structure evolves within both the cell boundaries in B and the structural component A. The degree of completion of the phase transformations within micro- and nano-volumes of the components determines the ultimate hysteretic characteristics of the material.

15 December 2021 in Materials
Verified
Journal Article
Open access
PDF file
ADAndrey Dormidontov
Andrey Dormidontov
NKNatalia B. Kolchugina
Natalia B. Kolchugina
NDNikolay A. Dormidontov
Nikolay A. Dormidontov
MZMark V. Zheleznyi
Mark V. Zheleznyi
ABAnna S. Bakulina
Anna S. Bakulina
NSNikolay N. Sysoev
Nikolay N. Sysoev
Observations of the surface domain structure (Kerr-effect), optical metallography, scanning electron microscopy (SEM-SE), and electron microprobe analysis (EPMA-SEM), measurements of major and minor magnetic hysteretic loops were used to study pseudo-single-crystal samples of (Sm,Zr)(Co,Cu,Fe)z alloys subjected to heat treatments to the high-coercivity state, which are used in fabricating sintered permanent magnets. Correlations between the chemical composition, hysteretic properties, structural components, domain structure, and phase state were determined for the concentration ranges that ensure wide variations of 4f-/4d-/3d-element ratio in the studied samples. The phase state formed by collinear and coherent phase components determines the high coercive force and ultimate magnetic hysteresis loops of the pseudo-single crystals. It was found that the 1:5 phase with the hexagonal structure (P6/mmm) is the matrix of the alloys for (Sm,Zr)(Co,Cu,Fe)z permanent magnets; the matrix undergoes phase transformations in the course of all heat treatments for the high-coercivity state. The heterogeneity observed with optical magnifications, namely, the observation of main structural components A and B, is due to the alternation, within the common matrix, of regions with modulated quasi-spherical precipitates and regions with hexagonal bipyramids (cellular phase) although, traditionally, many investigators consider the cellular phase as the matrix. It is shown that the relationship of volume fractions of structural components A and B that account for more than 0.9 volume fraction of the total, which is due to the integral chemical composition of the alloys, determines the main hysteretic performances of the samples. The Zr-rich phases, such as 5:19, 2:7, and 6:23, and a structural component with the variable stoichiometry (Sm(Co,Cu,Fe)3.5–5) that is almost free of Zr and contains up to 33 at% Cu, were found only within structural component A in quantities sufficient for EPMA analysis.

1 January 2017 in Moscow University Physics Bulletin
Verified
Journal Article
Closed access
PDF file
EME. V. Milov
E. V. Milov
ISI. A. Sipin
I. A. Sipin
VMV. N. Milov
V. N. Milov
AAA. S. Andreenko
A. S. Andreenko
IBI. A. Balan
I. A. Balan
Energy losses during alternating remagnetization of low-coercitivity resin-bonded magnets and commercially produced electrical steels were studied experimentally. The studies were conducted on several samples of resin-bonded magnets with different manufacturing technologies and samples of electrical steel sheets of various thicknesses. The static and dynamic magnetic properties of the samples were measured on a vibration magnetometer and a specially designed apparatus, respectively. It was found that the studied samples of bonded magnets have a relatively high level of hysteresis losses associated with high coercivity, which reaches a value of 4–5 Oe. At the same time, the remagnetization losses due to the Foucault currents in the bonded magnets are considerably lower than in electrical steels. The measurement results show that bonded magnets at high frequencies of remagnetization, especially in high-rpm motors, can be competitive in comparison with electrical steels.