A novel solid-state polyvinylchloride (PVC) membrane potentiometric dopamine-selective microsensor was constructed based upon dopamine-imprinted polymer (DOP-IP) used as the ionophore in the membrane structure. The optimum membrane composition was determined as 4% (w/w) DOP-IP, 69% (w/w) bis(2-ethylhexyl) sebacate (DOS), 26% (w/w) PVC, and 1% (w/w) potassiumtetrakis(4-chlorophenyl) borate (KTpClPB). The detection limit of the microsensor was determined to be 3.71 × 10–7 mol L–1. The microsensor exhibited a super-Nernstian response for dopamine over the concentration range of 10–6−10–1 mol L–1, with a short response time (<15 s) and a slope of 60.3 ± 1.3 mV per decade (R2: 0.9998) over seven weeks. The microsensor was effectively performed in a pH range of 4.0−8.0 and a temperature range of 5−30 °C. The microsensor has been successfully demonstrated for the rapid, accurate, selective and reproducible determination of dopamine in pharmaceutical formulations with the recovery of 104.3–104.8%. The obtained results were in good harmony with the UV-Vis results at a confidence level of 95%.