Lead-free ferroelectric materials are essential for environment-friendly solid-state cooling technology. In this respect, the electrocaloric effect of lead-free Ba0.8−xSr0.2SmxTiO3 (x = 0.01–0.05) ceramics has been investigated. The Rietveld refinement reveals that all the ceramics exhibit tetragonal symmetry and the tetragonality decreases for x > 0.03, which is the major reason behind the decrease in both isothermal entropy change and adiabatic temperature change. The degree of diffuseness parameter is enhanced by doping of Sm3+, which confirms the formation of polar nanoregion and the enhancement of the electrocaloric effect parameter by adding extra entropy. The relaxor behavior of the prepared samples is also confirmed by estimating the degree of deviation parameter from the curve. So, the temperature stability of the prepared ceramics is improved in a broad temperature window. The highest isothermal entropy change , adiabatic temperature change , and electrocaloric strength are found to be 1.230 Jkg−1 K−1, 0.862 K, and 0.028 73 K cm/kV at 316 K, respectively, for Ba0.77Sr0.2Sm0.03TiO3.
A coupled magnetostructural transition (MST) from a high-temperature low-magnetic -type hexagonal phase to a low-temperature high-magnetic -type orthorhombic phase, and the associated large magnetocaloric effect, are explored for the system. Room-temperature structural analysis is carried out to investigate the orthorhombic distortion of the hexagonal phase initiated by introducing at the site. The indirect isothermal magnetic measurement technique is employed to estimate the magnetocaloric effect across the coupled phase transition. Fascinatingly, a relatively large value of isothermal magnetic entropy change (Δ$S_{M}$) of (−12.02 ± 0.34) J ${\rm{kg}}^{-1}\;{\rm{K}}^{-1}$ at (332.5 ± 0.2) K and relative cooling power (RCP) of (119.6 ± 3.5) J ${\rm{kg}}^{-1}$ is achieved for the composition , for a field change of 30 kOe. The complex hysteresis behavior around the phase transition determines the efficiency of the material, which is revealed by both temperature- and field-sweep-rate dependence magnetization studies. Superheating (or supercooling) of the parent phase observed at higher temperature and field-sweep rates leads to broad thermal- and field-induced hysteresis. Lower sweep rates of temperature and magnetic field remove the quenching phenomenon across the MST and enhance the working efficiency. A large magnetocaloric effect and negligible variation of hysteresis with the temperature- and magnetic-field-sweep rates compared with other alloys makes this nominal low-cost material a promising candidate for practical solid-state cooling applications.
The advancement of magnetic materials with coupled magneto-structural phase transition (MST) to fulfill the ultimate objectives of practical solid-state cooling applications requires a better understanding of the hysteresis phenomenon linked across the phase transition region along with the large magnetocaloric parameters. For the present sample Mn0.65Ni0.65Fe0.70Si, the MST is associated with a sharp jump in magnetization along with a small thermal hysteresis of ∼13 K. A giant isothermal magnetic entropy change (|ΔSMmax|) of ∼37.6 J kg−1 K−1 at 299 K and effective refrigerant capacity (RCeffe) of ∼214.3 J kg−1 under ΔH = 30 kOe is obtained with excellent compatibility between the martensite and austenite phases. The geometrical compatibility condition, i.e., very small (∼0.55%) deviation of the middle eigenvalue (λ2) from unity justifies the observation of small hysteresis in the present material. The investigation of hysteresis behavior under different extents of the driving forces (temperature or magnetic field) reveals that both the driving forces trigger equally the phase transition and are responsible equivalently for the hysteresis phenomenon. The present study provides a pathway to understand the complexity of the hysteresis behavior, its impact on the reversibility of magnetocaloric effect, and its minimization by optimizing the geometrical compatibility condition between the austenite and martensite phases.
The (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 (0-3 type particulate) nanocomposites with x = 0.00, 0.02, 0.04, 0.06, 0.08, and 1.00 were prepared by the solid-state method. Cobalt ferrite crystallized into cubic crystal symmetry with an Fd3̄m space group. Strontium-substituted barium titanate crystallized into a tetragonal crystal structure with a P4mm space group. Field emission scanning electron microscopy and transmission electron microscopy techniques show the distribution of different sizes of particle. Polarization vs electric field curves show the highest maximum polarization (Pm) of 10.26 μC/cm2, remnant magnetization (Pr) of 11.70 μC/cm2, and coercivity (Ec) of 19.95 kV/cm for x = 0.04 composition at 35 kV/cm. However, it is smaller than the Ba0.8Sr0.2TiO3 phase (Pm = 16.86 μC/cm2, Pr = 13.20 μC/cm2, and EC = 10.80 kV/cm). The highest dielectric constant of around 9800 was found for x = 0.04 composition, with a very small dielectric loss factor of about 0.02, i.e., less than even 2%. This is ∼10 times compared to that of Ba0.8Sr0.2TiO3 (BSTO), which has been explained by considering interaction at the interface of CoFe2O4 (CFO) and BSTO, leakage current, and variation of the lattice parameter of BSTO in (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 nanocomposite. The magnetic hysteresis loops show squeezing near the origin. The magnetic parameters like coercivity, remnant magnetization, and saturation magnetization increased with the increase in the CoFe2O4 weight fraction. Magnetic interaction between surfaces of magnetic CFO and non-magnetic BSTO is evident from the ΔH vs M plots, and it also evidences the magnetism at the surface of BSTO due to uncompensated spins.