This work shows the possibility of obtaining Al2O3–ZrO2–Y2O3medical ceramics from powders synthesized by nanospray drying. The powder is spheres with a uniform distribution of components: mixed...
The composite powders of aluminium and zirconium oxides containing 10, 50 and 90 mol % Al 3+ without a stabilizer have been obtained from suspensions using a spray drying method. The powders obtained at equal mole ratios of zirconium and aluminum in the original solution (0.5:0.5 mol/l) have the largest contents of cubic and tetragonal phases of ZrO2, strictly uniform distribution of phases and the largest value of the specific surface area. The particles with two different morphologies have been obtained: crystalline particles of oxides uniformly distributed in a particle and particles in membrane consisting of zirconium oxide or mixed oxides. It has been experimentally shown that zirconium oxide stabilizes the amorphous phase of aluminum oxide, and aluminum oxide increases the temperature of crystallization of zirconium oxide.
—An yttrium aluminum garnet (YAG) luminescent ceramic activated by Ce3+ has been obtained by uniaxial static pressing followed by sintering in air at a temperature of 1650°C. The initial phosphor powder was characterized and the linear shrinkage dynamics studied. The morphological, elastoplastic, and optical-luminescent properties of the obtained YAG:Ce ceramic samples were studied. The technological mode for manufacturing ceramics of this type with a density of at least 98% and luminescence efficiency of 45% was determined.