Friction surfacing (FS) is a solid-state layer deposition process for metallic materials at temperatures below their melting point. While the bonding of the deposited layers to the substrate is proven suitable for coating applications, so far the mechanical properties of additively manufactured stacks have not been systematically investigated. In particular, the effect of successive deposited FS layers, i.e., repetitive thermo-mechanical loading, on the interface properties as well as anisotropy and strength of the deposited stack is unknown. For this purpose, the mechanical properties of FS deposited multi-layer stacks from dissimilar aluminum alloys have been investigated, characterizing layer-to-layer as well as layer-to-substrate bonding interfaces via micro-flat tensile testing. Furthermore, directional dependencies in the stack and failure mechanisms are analyzed. The results show a homogeneous, fine-grained microstructure with average grain sizes between 4.2 and 4.6 μ m within the deposited material. The resulting tensile properties with no significant directional dependency present an ultimate tensile strength between 320 and 326 MPa exceeding the strength of the AA5083 H112 consumable base material. No difference was obtained in terms of layer-to-layer or layer-to-substrate interface strength. Furthermore, homogeneous hardness was observed within the deposited structure, which is in the range of AA5083 base material’s hardness of 91 HV. The results indicate that the FS process in conjunction with the material used is suitable for additively generated structures and highlight the potential of this solid-state layer deposition technology.
The process variant of friction surfacing (FS) depositing multiple layers on top of each other is known as multi-layer friction surfacing (MLFS). Due to the solid-state nature of the process, re-heating is significantly reduced compared to common fusion-based AM techniques. The work gives a detailed and fundamental insight into the microstructure along the MLFS build direction for two different aluminum alloys and different process parameters. Focusing on the grain size distribution and recrystallization ratio, the stacks show a higher degree of recrystallization and finer grains at the interfaces. The observed grain sizes at the interfaces were 2.0 µm (AA5083) and 1.1 µm (AA2024), and 5.8 µm (AA5083) and 3.1 µm (AA2024) at the layer center. For the non-precipitation-hardenable alloy (AA5083), the local microstructural trend could be related to the hardness distribution along the stacks, i.e., a slightly higher hardness at the layer interfaces (95 HV) compared to the layer center (90 HV). The relationship is more complex for precipitation-hardenable alloys (AA2024), which show a rise in hardness between 40 HV0.2 and 45 HV0.2 along the stack height. The effect of subsequent layer depositions on the microstructure and hardness is discussed and a distinctive grain size distribution along the build direction was shown to be a fundamental characteristic.