22 July 2011 in Advanced Materials
21 December 2005 in Physical Review B
, which has a monoclinic structure, shows weak ferromagnetism below and a ferroelectric transition at accompanied by hysteresis. We have determined the structure and energetics of with ferromagnetic and antiferromagnetic ordering by means of first-principles density functional theory calculations, based on pseudopotentials and a plane-wave basis. The noncentrosymmetric monoclinic structure is found to be lower in energy than the orthorhombic structure, supporting the biferroic nature of .
1 November 1983 in Journal of Applied Physics
Ferroelectric films of lead zirconate titanate (PZT) have been fabricated by rf planar magnetron sputtering. Films having a resistivity >106 Ω cm and a dielectric constant >800 at 300 K have been achieved using 100% oxygen as a sputtering medium, 10% excess PbO added to the target, and appropriate post‐deposition annealing. The sputtering rate is in the range 0.2–1.0 μm/h and varies with sputtering pressure and substrate temperature. Post‐deposition annealing affects both crystallinity and grain size, but incipient crystallization formed only in as‐grown films deposited at substrate temperatures >400 °C is essential for this process to be effective. A clear ferroelectric transition is observed at 350 °C, while the activation energy for dc conductivity of around 0.8 eV is consistent with bulk properties of PZT. The spontaneous polarization and coercive field measured from ferroelectric hysteresis loops is 20.75 μC/cm2 and 10 kV/cm, respectively. The optical transmittance of the films is determined by a Pb–Pb charge transfer band near 400 nm and this is a sensitive test of film stoichiometry.
1 June 1993 in Journal of Applied Physics
Polycrystalline SrTiO3 thin films having perovskite structure were prepared by the metallo‐organic solution deposition technique on platinum coated silicon and bare silicon substrates. Crack free and crystalline films with uniform composition and thickness were fabricated by spinning and post deposition rapid thermal annealing at a low temperature of 550 °C for 60 s. The films exhibited good structural, dielectric, and insulating properties. The dielectric constant was found to depend on film thickness and annealing temperature. The small signal dielectric constant and dissipation factor at a frequency of 100 kHz were 225 and 0.008, respectively, for a 0.8‐μm‐thick film annealed at 700 °C for 60 s. The frequency dependence of the dielectric constant and the dielectric loss was also studied. The measurement of the current‐voltage (I‐V) characteristics on films in metal‐insulator‐metal configuration indicated the conduction process to be bulk limited. The I‐V characteristics were ohmic at low fields and space‐charge limited at high fields. Room temperature resistivity of 1013 Ω cm and leakage current density of less than 10−8 A/cm2 were obtained for a 0.8‐μm‐thick film at an applied electric field of 200 kV/cm, establishing good insulating behavior. The interfacial properties of gold‐strontium titanate‐silicon structures were studied experimentally by measuring the capacitance‐voltage (C‐V) characteristics. The C‐V curves exhibited anomalous frequency dispersion behavior and a hysteresis phenomenon. The hysteresis in the C‐V curve was found to be about 0.8 V and of a charge injection type. The density of interface states recharged during the bias cycle in hysteresis measurement was estimated to be of the order of 8.3×1011 cm−2. The density of interface states at the flatband voltage was found to have a value of 1.38×1012 eV−1 cm−2. For a 0.5‐μm‐thick SrTiO3 film, a unit area capacitance of 3.5 fF/μm2 and a charge storage density of 36.7 fC/μm2 were obtained at an applied electric field of 200 kV/cm. These measured parameters place SrTiO3 as one of the suitable dielectric material for dynamic random access memory applications.
1 January 2001 in Solid-State Electronics
1 June 1994 in Journal of Materials Research