1 July 2020 in Journal of Environmental Management
1 October 2021 in Magazine of Concrete Research
The compressible packing model (CPM), which is a method for designing aggregate gradation, was used to calculate the packing density of quartz aggregate. The aggregate gradation of ultra-high-performance concrete (UHPC) was optimised using the CPM. The number of interfaces between the aggregates and cement was determined using Image-Pro Plus software. The CPM modified using the equation Y = 0·60073X + 0·20551 was found to calculate the packing density of quartz aggregate accurately. The compressive strength of the UHPC was found to be positively correlated with the packing density of the aggregate: an increase in the packing density led to a compressive strength increase from 97·9 MPa to 124·1 MPa, an increase of 26·7%. The flexural strengths of the material was found to be sensitive to the number of interfaces: the smaller the number of interfaces, the greater the flexural strength. The specimen with an interface length of 5·56 mm/mm2 had the smallest flexural strength (21·5 MPa) and the specimen with an interface length of 3·596 mm/mm2 had the largest flexural strength (25·9 MPa). It is recommended that, when designing aggregate gradation, a gradation with high density should be selected and the proportion of small-size aggregates should not be too large.
12 April 2022 in Journal of Advanced Concrete Technology
The hydration characteristics and mechanical properties of basic magnesium sulfate (BMS) cement containing steel slag (SS) are studied in the work. The heat release of the composite binders during hydration process was monitored, the phase compositions of hydration products were analyzed, the microstructures of hardened pastes were investigated, moreover, the compressive strength was tested. The results show that the hydration exothermic rate of BMS is slowed and the cumulative heat of BMS is suppressed by SS addition. The incorporation of SS leads to the formation of C-S-H, CaSO4•2H2O and Mg(OH)2, and suppresses the formation of 5-1-7 phase. Compared to plain BMS, the pore structure of the composite paste with SS addition is much coarser, the crystallization and growth of Mg(OH)2 lead to the occurrence of microcrack and large pores of the paste. The mechanical property of BMS is decreased by SS addition, especially when the content of SS addition reaches 20%, the compressive strength is significantly weakened in all tested ages.