This research explored the temperature dependence magnetization, magnetocaloric effect, and critical field analysis of Nd0.7−xLaxSr0.3MnO3 (x = 0.0, 0.1, 0.2 and 0.3) manganites samples synthesized through solid state reaction route. The substitution of La3+ at Nd3+ site enhances the A-site average ionic radius ( ) from 1.321 Å (for x = 0.0) to 1.348 Å (for x = 0.3). An increase in reduced the internal chemical pressure inside the lattice such that the Mn–O–Mn bond angle approached 180°. In addition, an increase in Mn–O–Mn bond angle supresses the spin-lattice interaction, which consequently reduces the change in maximum magnetic entropy at the magnetic transition temperature. This implies that variation of A-site average ionic radius influences the change in maximum magnetic entropy. The critical behavior of the manganite samples was addressed based on the data of magnetization measurements around the transition temperature TC. Various techniques such as modified Arrott plot, a Kouvel–Fisher method, and critical isotherm analysis were used to measure the values of the ferromagnetic transition temperature TC, as well as the critical exponents of β, γ, and δ. The magnetic order parameter is very well obeyed with scaling relation with change in magnetic entropy.
Calcium Barium Titanate ceramics were synthesized and investigated to assess the effect of Ba2+ substitution on the structural, vibrational, optical, and ferroelectric properties. A single-phase perovskite structure with a gradual peak shift toward lower 2θ values is confirmed by X-ray diffraction. An increase in crystallite size from 165 to 244 nm with decreasing dislocation density and variable microstrain was revealed by Williamson-Hall and Debye-Scherrer analyses. FTIR and Raman spectroscopy showed characteristic Ti-O vibrational modes, with band shifts reflecting local lattice distortion and enhanced symmetry. Optical absorption and Tauc plots indicated a systematic band gap reduction from 3.50 eV to 3.10 eV, accompanied by an increase in Urbach energy (0.32-0.49 eV), confirming the role of defect states in band tailing. Optical conductivity spectra exhibited enhanced electronic transitions in the UV region. Ferroelectric P-E hysteresis measurements demonstrated a transformation from incipient ferroelectricity in CaTiO3 to well defined loops in Ba-substituted samples, with optimum remanent polarization (116.912 µC/cm2) and highest coercive field (-79.385 V/cm). These results establish Ba substitution as an effective strategy to tailor the structural perfection, dielectric response, and optical band structure of CaTiO3 ceramics, making CBT compositions promising for multifunctional optoelectronic and ferroelectric device application.