View All Publications
11 March 2011 in Oxidation of Metals
Verified
Journal Article
Open access
PDF file
JPJesper Pettersson
Jesper Pettersson
NFNicklas Folkeson
Nicklas Folkeson
LJLars-Gunnar Johansson
Lars-Gunnar Johansson
JSJan-Erik Svensson
Jan-Erik Svensson
The oxidation of 304-type (Fe18Cr10Ni) austenitic stainless steel was investigated at 500 and 600 °C in 5% O2 + 40% H2O. Prior to exposure the samples were sprayed with KCl, K2CO3 or K2SO4, the amount of salt corresponding to 1.35 μmol K+/cm2. For reference, salt-free samples were exposed in 5% O2 + 40% H2O and in 5% O2 (N2 was used as carrier gas). The oxidized samples were analyzed with SEM/EDX, XRD, IC and FIB. KCl and K2CO3 strongly accelerate the corrosion of 304L while K2SO4 has little influence on the corrosion rate and on the morphology of the corroded surface. KCl and K2CO3 react with the chromium-rich oxide on the sample surface, forming K2CrO4. The resulting chromium depletion of the protective oxide causes rapid oxidation and the formation of a thick duplex scale consisting of an outer hematite layer and a inner layer made up of FeCrNi spinel-type oxide. The differences in the corrosivity of the three salts are directly connected to their ability to form chromate on the surface and, hence, to the relative stability of the corresponding leaving groups (HCl, CO2 and SO3).

27 April 2012 in Oxidation of Metals
Verified
Journal Article
Open access
PDF file
SKS. Karlsson
S. Karlsson
JPJ. Pettersson
J. Pettersson
LJL. -G. Johansson
L. -G. Johansson
JSJ. -E. Svensson
J. -E. Svensson
The influence of KCl, NaCl and CaCl2 on the oxidation of 304-type (Fe18Cr10Ni) stainless steel at 600 °C in 5 %O2 + 40 %H2O was investigated. Prior to exposure, a small amount of the preferred salt (cation equivalent: 1.35 μmol/cm2) was deposited on the samples. Exposure time was 1–168 h. The oxidized samples were analyzed by SEM/EDX, XRD, FIB and IC. The presence of KCl and NaCl strongly accelerates high temperature corrosion of 304L. Corrosion attack is initiated by the formation of alkali chromate through the reaction of alkali with the protective oxide. Chromate formation is a sink for chromium in the oxide and leads to a loss of its protective properties. Subsequently a rapidly growing scale forms, consisting of an outer hematite layer with chromate particles on top and an inner spinel oxide layer. In contrast to NaCl and KCl, CaCl2 is not very corrosive. At temperature, CaCl2 is rapidly converted to CaO. Small amounts of CaCrO4 form where CaO is in direct contact with the scale. CaO also reacts with the scale to form Ca2Fe2O5.

11 June 2018 in Nature Materials
Verified
Journal Article
Closed access
PDF file
NMN. Mortazavi
N. Mortazavi
CGChristine Geers
Christine Geers
MEM. Esmaily
M. Esmaily
VBV. Babic
V. Babic
MSM. Sattari
M. Sattari
LJL. G. Johansson
L. G. Johansson