Metallic biopolymer-based nanomaterials have emerged as a sustainable and versatile class of hybrid nanostructures, offering environmentally benign alternatives to conventionally synthesized nanomaterials.
This study reports the development of an environmentally benign photocatalyst through the sericin‐mediated green synthesis of zinc oxide nanoparticles (SS‐ZnO NPs), utilizing waste silk byproduct sericin. Sericin acted as both a reducing and stabilizing agent. The synthesized SS‐ZnO NPs were comprehensively characterized using UV–vis spectroscopy, x‐ray diffraction (XRD), scanning electron microscopy (SEM), energy‐dispersive x‐ray spectroscopy, dynamic light scattering, and zeta potential analysis. The absorption peak at 340.0 nm validated the successful formation of SS‐ZnO NPs. The SS‐ZnO NPs exhibited a hexagonal wurtzite crystal structure with an average crystallite size of 82.66 nm. SEM analysis revealed a distinctive flower‐like morphology, and the average zeta potential was measured at +8.82 mV, indicating moderate colloidal stability. Photocatalytic performance was evaluated through the degradation of methyl orange (MO) dye. The highest degradation efficiency was observed at a dye concentration of 10 ppm, pH 4, and catalyst dosage of 0.2 g L −1 , yielding a maximum degradation rate constant of 0.0432 min −1 . The acidic conditions significantly favor the photocatalytic process compared to neutral and alkaline environments. The catalyst's stability after the first cycle of MO degradation was also assessed by conductivity and XRD measurements. Thus, sericin is a potential chemical species for synthesize effective ZnO NPs photocatalyst.
Lignin, due to its structural diversity and biodegradability has emerged as a promising alternative to hazardous synthetic materials in multidisciplinary research area. The aim of this paper is to evaluate the lignin potential in value-added applications to be exact zinc oxide nanoparticle synthesis. First, lignin was extracted from coconut husk via sonochemical route in alkaline medium. Afterward, lignin-zinc oxide hybrid nanoparticles (L-ZnO NPs) were synthesized by the reaction of zinc acetate dihydrate salt and lignin, where lignin acts as bioreducing and capping agent. The synthesized lignin and L-ZnO NPs were characterized by UV-Vis spectroscopy, FTIR Spectroscopy, XRD and FESEM analysis. All the identification tests supported the existence of lignin and L-ZnO NPs. The XRD and SEM images disclosed the formation of hexagonal wurtzite shape L-ZnO NPs having mean diameter ≈ 77.76 nm. The antibacterial efficacies of the L-ZnO NPs were assessed against both gram-negative E. coli and gram-positive S. aureus bacteria, employing standard controls and the well diffusion method. The L-ZnO NPs exhibited marvelous bactericidal action against the test microorganisms displaying sufficient zone of inhibition. The photocatalytic performance of the L-ZnO NPs was observed by methylene blue (MB) dye degradation test under UV light irradiation. The UV-Vis absorbance and conductivity tests suggested that the L-ZnO NPs has noticeable photocatalytic efficiency on MB dye degradation. Therefore, the synthesized L-ZnO NPs possess excellent versatile properties and it can be used in medicinal applications and environmental management.
The structural geometry of the predominant sodium chloride (NaCl) phase was examined by powder X-ray diffraction (XRD), followed by whole powder pattern fitting (WPPF) to evaluate the crystallographic profile. The prominent crystalline phase exhibited cubic symmetry, with lattice constants a=b=c= 5.6231 Å and angles α=β=γ= 90°. The prominent reflection at 2θ= 32.08° was indexed to the (200) crystallographic plane. The whole powder pattern fitting (WPPF) method identified halite as the predominant crystalline phase, with a modeled crystalline phase fraction of 100.0 % assigned to NaCl. Multiple established methods were applied to assess and evaluate the average crystallite size, with estimated values ranging from 101.21 to 290.29 nm depending on the adopted diffraction peak-broadening model. The crystallographic analysis revealed a dislocation density of 9.76 × 10⁻5 nm− 2, crystallinity index of 1.112 with a percentage of crystallinity of 86.03 %, an atomic packing factor of 65.88 %, a lattice volume of 177.797 Å3, a unit cell density of 2.183 g/cm3 and a specific surface area of 27.16 m2/g. Microscopic imaging revealed predominantly cubic and faceted particles with well-defined boundaries. The TEM revealed predominantly cubic and faceted particles with well-defined boundaries, while SAED patterns were consistent with highly crystalline halite. The EDS showed Na and Cl contents of 47.83 and 52.17 at %, respectively, indicating a NaCl dominated elemental composition. Overall, the results demonstrate a predominantly halite-type cubic structure and faceted morphology, while the relatively high WPPF residuals warrant cautious interpretation of the refined structural and microstructural parameters.