This present study aimed to clarify the effect of contact scale and surface topography of substrates with different roughnesses on the actual contact area, tangential stiffness, and tangential deformation of the substrate at micro- and macro-scales via finite element method (FEM) simulations, as well as the final tribological performances of MoS2 coatings by experiments. The MoS2 coatings were deposited on stainless steel (SS) substrates with different roughnesses, and the settings in the simulation models were based on the roughness of the SS substrates. The predicted tribological behavior of the simulation results was confirmed by the morphological and compositional analysis of the wear track using scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDS), 3D profilometer, and Raman spectroscopy. The results showed that the substrate with a surface roughness of Ra 600 nm (R600), coated by MoS2 nanosheets, exhibited excellent tribological properties at both micro- and macro-scales. At the micro-scale, the lubrication lifetime of R600 was as long as 930 cycles, while the substrates with surface roughnesses of Ra 60 nm (R60) and Ra 6 nm (R6) had a lubrication lifetime of 290 cycles and 47 cycles, respectively. At the macro-scale, the lifetime of the substrate R600 was 9509 cycles, which was nearly six times longer than the 1616 cycles of substrate R60. For the rough surface of substrate, the surface grooves could not only effectively preserve the lubricant but also continuously release them, ensuring that the lubricants with low shear strength were always present in the contact interface. It was further verified that the high surface roughness of the substrate reduced friction and wear by reducing the actual contact area and enhancing the tangential stiffness of asperities, thereby prolonging the lubrication lifetime. The wear mechanisms were discussed in terms of the morphology and chemical composition of the wear tracks.
The structure and morphology of Cu films deposited by DC magnetron sputtering on silicon and stainless-steel substrates at different deposition temperatures of −140 °C, −95 °C, −55 °C, 25 °C (RT), 50 °C, and 200 °C were investigated by X-ray diffraction (XRD), scanning electron microscopy (SEM), and atomic force microscopy (AFM). It was found that all Cu films presented strong orientation of the (111) and (200) peaks. The Cu films deposited at low temperatures (lower than −55 °C) showed the bilayer structures, in which the upper layer appeared to be a loose and porous structure and the lower layer near the substrate had a fine and dense structure that consisted of small grains. In addition, the Cu films deposited at low temperatures could be observed a large roughness. The roughness tended to decline and then increase with the rising of deposition temperature. The ball-on-disc reciprocating sliding tribometer was employed to evaluate the tribological behaviors of the Cu films at current-carrying levels of 0 A, 0.5 A, and 1.0 A. The results revealed that the Cu films deposited at low temperatures exhibited outstanding current-carrying friction performance and low electrical contact resistance (ECR), peeling only at 0.5 A and 1.0 A. Nevertheless, the Cu films deposited at the relatively high temperature exhibited oxidative wear caused by electric arc ablation at 0.5 A and 1.0 A. Additionally, the wear mechanism was discussed in terms of the structure and morphology of the wear track and formation of the tribo-film.