Advanced material composite of nanocarbons and metal-based materials provides a synergistic effect to obtain excellent electrochemical charge-storage performance and other properties. Herein, 3D porous carbon-metal oxynitride nanocomposites with tunable carbon/metal and oxygen/nitrogen ratio are synthesized uniquely by simultaneous ablation from two different targets by single-step pulsed laser deposition at room temperature. Co-ablation of titanium and vanadium nitride targets together with graphite allowed us to synthesize carbon-metal oxynitride porous nanocomposite and exploit them as a binder-free thin film supercapacitor electrode in aqueous electrolyte. We show that the elemental composition ratio and hence the structural properties can be tuned by selecting target configuration and by manipulating the ablation position. We investigate how this tuning capability impacts their charge-storage performances. We anticipate the utilization of as-synthesized various composites in a single PLD production run as next-generation active materials for flexible energy storage and optoelectronic applications.
This study presents a simple route to prepare binder-free activated amorphous carbon nanofoam, which is explored as an electrochemical energy storage electrode.
By depositing zinc nitride on bare Zn, the present study showcases that nitride coating suppresses the insulating oxide/hydroxide layer formation, controls the growth of Zn nucleation and forms a uniform network of Zn nanostructures. Hence, an aqueous zinc-ion hybrid micro-capacitor delivers better charge-storage performance and long lifespan with capacitance retention of 110% after 10000 cycles. Corresponding author email: subrata.ghoshk@rediffmail.com or subrata.ghosh@upes.ac.in (S.G.) and carlo.casari@polimi.it (C.S.C.)
In this communication, we demonstrate an aqueous supercapacitor based on self-standing, porous, columnar, and 26 μm thick activated carbon nanofoam. The device delivers areal (volumetric) capacitance of 95.4 mF/cm2 (18.3 F/cm3) at 2 mA with retention of 103% at 20 mA and achieves 1V voltage compared to pristine and annealed ones.