Ground tire rubber (GTR) was devulcanized by microwaves at the same heating rate (constant power) and different times of exposure. The devulcanized rubber (DV-R) and untreated GTR were characterized physically and thermally. Composite materials were prepared from different proportions of the GTR, which was used as a filler, and the DV-R, which was used as part of the styrene butadiene rubber (SBR) matrix, and by varying the exposure time of the microwave power. These composites were compared with a control sample that was prepared from virgin SBR. The sol content (soluble part) and Fourier transform infrared spectroscopy (FTIR) analyses of the devulcanized samples were examined to define the efficiency of devulcanization. The cure characteristics and tensile properties of the SBR composites were researched. In this study, it was found that using DV-R as part of the rubber matrix produced much better properties than using GTR as a filler, thereby showing the significant benefits of microwave devulcanization. At the DV-R content of 50 phr, the elongation at break of the DV-R 5 min/SBR composites increased to 445.06% from 217.25% for the GTR/SBR composites, i.e., the elongation at break was enhanced by 105% by the devulcanization of GTR. Scanning electron microscopy (SEM) photographs displayed a better interface coherence between the DV-R 5 min and SBR matrix than the GTR/SBR composites.
This article investigates the impact of addition various types of nanoparticles with different structural, dimensional, and morphological properties on the interphase region formed between the particle/matrix and the curing behavior of the epoxy affect the nanocomposite material properties. For this purpose, epoxy nanocomposites (NCs) were produced by adding multi-walled carbon nanotube (MWCNT) and alumina (Al2O3) nanoparticles (NPs) into the epoxy matrix at different rates (0.5–2.0 wt.%). The effects of the particle/matrix interaction on the properties of the composite have been revealed by chemical, thermal, mechanical analyzes and microstructure investigations. An increase in the absorption density, which reveals the physical interaction of nanoparticles with the epoxy matrix, was observed in Fourier-transform infrared spectroscopy. Absorption vibration peak intensities in nanocomposite samples were at most 1.0 wt.% Al2O3 and 1.25 wt.% CNT added nanocomposites. It was observed that the Tg value increased depending on the number of nanoparticles. The addition of Al2O3 increased Tg values more than CNT. Besides, the mechanical properties of NCs were determined by tensile tests. The highest increase in mechanical properties was achieved by adding 1.25 wt.% CNT and 1.0 wt.% Al2O3, respectively. Mechanical properties tended to decrease at higher addition rates. The shape, size, amount, and distribution of nanoparticles added into the epoxy matrix directly affected the NCs' properties. It has been determined that homogeneously dispersed spherical Al2O3 nanoparticles are more effective than fiber-shaped CNTs in the properties of NCs.