Patrick Desjardins

Patrick Desjardins

Auto-generated profile, based on publicly available information

Patrick Desjardins

École Polytechnique de Montréal Regroupement Québécois sur les Matériaux de Pointe (RQMP) and Département de Génie Physique P.O. Box 6079, Station Centre-Ville, Montréal, Québec H3C 3A7, Canada

Research Focus & Metrics

Academic Career Length

37Years (1990-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
20 April 2006 in Journal of Vacuum Science & Technology A
Verified
Journal Article
Closed access
PDF file
SGS. Gaudet
S. Gaudet
CDC. Detavernier
C. Detavernier
AKA. J. Kellock
A. J. Kellock
PDP. Desjardins
P. Desjardins
CLC. Lavoie
C. Lavoie
A systematic study of the thermally induced reaction of 20 transition metals (Ti, Zr, Hf, V, Nb, Ta, Cr, Mo, W, Mn, Re, Fe, Ru, Co, Rh, Ir, Ni, Pd, Pt, and Cu) with Ge substrates was carried out in order to identify appropriate contact materials in Ge-based microelectronic circuits. Thin metal films, nominally 30nm thick, were sputter deposited on both amorphous Ge and crystalline Ge(001). Metal-Ge reactions were monitored in situ during ramp anneals at 3°Cs−1 in an atmosphere of purified He using time-resolved x-ray diffraction, diffuse light scattering, and resistance measurements. These analyses allowed the determination of the phase formation sequence for each metal-Ge system and the identification of the most promising candidates—in terms of sheet resistance and surface roughness—for their use as first level interconnections in microelectronic circuits. A first group of metals (Ti, Zr, Hf, V, Nb, and Ta) reacted with Ge only at temperatures well above 450°C and was prone to oxidation. Another set (Cr, Mo, Mn, Re, Rh, Ru, and Ir) did not form low resistivity phases (<130μΩcm) whereas no reaction was observed in the case of W even after annealing at up to 1000°C. We found that Fe, Co, Ni, Pd, Pt, and Cu were the most interesting candidates for microelectronic applications as they reacted at relatively low temperatures (150–360°C) to form low resistivity phases (22–129μΩcm). Among those, two monogermanides, NiGe and PdGe, exhibited the lowest resistivity values (22–30μΩcm) and were stable over the widest temperature window during ramp anneals. In passing, we note that Cu, Ni, and Pd were the most effective in lowering the crystallization temperature of amorphous Ge, by up to 290°C for our typical ramp anneals at 3°Cs−1.

1 May 2006 in Applied Physics Letters
Verified
Journal Article
Closed access
CAC. M. Aguirre
C. M. Aguirre
SAS. Auvray
S. Auvray
SPS. Pigeon
S. Pigeon
RIR. Izquierdo
R. Izquierdo
PDP. Desjardins
P. Desjardins
RMR. Martel
R. Martel
High performance organic light-emitting diodes (OLEDs) were implemented on transparent and conductive single-wall carbon nanotube sheets. At the maximum achieved brightness of 2800cdm−2 the luminance efficiency of our carbon nanotube-based OLED is 1.4cdA−1 which is comparable to the 1.9cdA−1 measured for an optimized indium tin oxide anode device made under the same experimental conditions. A thin parylene buffer layer between the carbon nanotube anode and the hole transport layer is required in order to readily achieve the measured performance.

23 October 2000 in Physical Review Letters
Verified
Journal Article
Closed access
PDF file
AVA. Vailionis
A. Vailionis
BCB. Cho
B. Cho
GGG. Glass
G. Glass
PDP. Desjardins
P. Desjardins
DCDavid G. Cahill
David G. Cahill
JGJ. E. Greene
J. E. Greene
The two-dimensional (2D) to three-dimensional (3D) morphological transition in strained Ge layers grown on Si(001) is investigated using scanning tunneling microscopy. The initial step takes place via the formation of 2D islands which evolve into small ( ≃180 Å) 3D islands with a height to base diameter ratio of ≃0.04, much smaller than the 0.1 aspect ratio of {105}-faceted pyramids which had previously been assumed to be the initial 3D islands. The “prepyramid” Ge islands have rounded bases with steps oriented along 〈110〉 and exist only over a narrow range of Ge coverages, 3.5–3.9 monolayers.

24 March 2005 in Plasma Processes and Polymers
Verified
Journal Article
Closed access
PDF file
PGPierre‐Luc Girard‐Lauriault
Pierre‐Luc Girard‐Lauriault
FMFackson Mwale
Fackson Mwale
MIMihaela Iordanova
Mihaela Iordanova
CDCaroline Demers
Caroline Demers
PDPatrick Desjardins
Patrick Desjardins
Michael WertheimerMichael Wertheimer
Michael Wertheimer

28 July 1997 in Applied Physics Letters
Verified
Journal Article
Closed access
PDF file
HMH. Marchand
H. Marchand
PDP. Desjardins
P. Desjardins
SGS. Guillon
S. Guillon
JPJ.-E. Paultre
J.-E. Paultre
ZBZ. Bougrioua
Z. Bougrioua
RMR. A. Masut
R. A. Masut
The metalorganic vapor phase epitaxy of coherent self-assembled InAs islands on InP(001) is demonstrated. Samples are characterized using transmission electron microscopy and photoluminescence (PL) spectroscopy at 77 K. The deposition of ∼2.4–4.8 monolayers (ML) of InAs at 500° C followed by a 30 s growth interruption results in the formation of coherent islands whose average diameter is 30–35 nm with a standard deviation of 8 nm and whose areal density is (3–4)×1010 cm−2. The PL emission is centered at 0.79 eV and has a full width at half maximum (FWHM) of 90 meV. When the nominal deposited thickness is increased to ∼9.6 ML, the average island diameter increases to ∼120 nm while the areal density decreases to ∼109 cm−2. The resulting PL is then centered at 0.83 eV with a FWHM of 130 meV and also displays a peak at 1.23 eV which is attributed to an InAs wetting layer ∼ 2 ML in thickness.

4 July 2008 in Nano Letters
Verified
Journal Article
Closed access
EAE. Adam
E. Adam
CAC. M. Aguirre
C. M. Aguirre
LML. Marty
L. Marty
BSB. C. St-Antoine
B. C. St-Antoine
FMF. Meunier
F. Meunier
RMR. Martel
R. Martel